This document is a federal specification section (Section 09 96 00) detailing requirements for high-performance coatings for the DDG(X) LBTS WP3: E-Campus project. The specification provides comprehensive technical guidance for coating applications, focusing on epoxy and polyurethane coatings for various substrates including ferrous and galvanized metal surfaces. Key requirements include using Master Painters Institute (MPI) standards, submitting detailed product data and color samples for government approval, and ensuring specific coating application techniques and film thickness measurements.

The specification mandates precise surface preparation, including removing rust, mill scale, grease, and oil from metal surfaces, and specifies coating application methods such as brush, roller, and spray techniques. For exterior concrete walls, the coating must match Benjamin Moore's Red Rock color (Number 2005-10). Environmental conditions are strictly controlled, with painting prohibited below 50 degrees F or above 95 degrees F, and requiring proper ventilation and safety precautions during application. The government reserves the right to conduct field tests to verify coating thickness and quality, with contractors required to repair or replace any unsatisfactory work at no additional cost.

View the file

Other files

File Type Posted
N4008525R35000007CLEAN.pdf PDF
Amendment 0006 Energy Campus Site Photos 4of4.pdf PDF
Amendment 0006 Energy Campus Site Photos 2of4.pdf PDF
Amendment 0006 Energy Campus Site Photos 1of4.pdf PDF
AMENDMENT 0006.pdf PDF
Amendment 0006 Energy Campus Site Photos 3of4.pdf PDF
Amendment 0005 DDG(X) WP3_Dwgs.pdf PDF
Amendment 0005 PS-77-001.0_SD2_PNY B77 POD_Shop Drawing Submittal.pdf PDF
Amendment 0005 CMT Services Group - Navy Yard - Additional Water Results.xlsx XLSX spreadsheet
N4008525R3500 Amendment 0005 final.pdf PDF
Amendment 0005 3G010 - UTILITY COORDINATION AND SEQUENCE OF CONSTRUCTION.pdf PDF
Amendment 0005 02 61 13 - EXCAVATION AND HANDLING OF CONTAMINATED MATERIAL.pdf PDF
N4008525R3500 Amendment 0004.pdf PDF
DDG(X) WP3_Amendment 0003_Continuation Sheet.pdf PDF
N4008525R3500 Amendment 0003.pdf PDF
Amendment 0003 Attachment 1.pdf PDF
DDG(X) WP3_Amendment 0003_Spec Section 22 25 00.pdf PDF
DDG(X) WP3_Amendment 0003_Spec Section 02 61 13.pdf PDF
Amendment 0003 ATTACHMENT G - PRICE SCHEDULE.pdf PDF
DDG(X) WP3_Amendment 0003_Dwgs_Signed.pdf PDF
N4008525R3500 Amendment 0002.pdf PDF
Amendment 0002 Site-Visit Sign In Sheets.pdf PDF
Amendment 0001 Site Visit Information.pdf PDF
N4008525R3500 Amendment 0001.pdf PDF
N4008525R3500 Drawings.pdf PDF
ATTACHMENT E - SMALL BUSINESS PARTICIPATION COMMITMENT DOCUMENT (SPCD).pdf PDF
ATTACHMENT G - PRICE SCHEDULE.pdf PDF
ATTACHMENT F - SMALL BUSINESS SUBCONTRACTING PLAN.pdf PDF
ATTACHMENT B - CONSTRUCTION EXPERIENCE PROJECT DATA SHEET.pdf PDF
Solicitation - N4008525R3500 (final).pdf PDF
ATTACHMENT C - PAST PERFORMANCE QUESTIONAIRE (PPQ).pdf PDF
N4008525R3500 Specs.pdf PDF
ATTACHMENT H - PIEE VENDOR ACCESS INSTRUCTIONS.pdf PDF
ATTACHMENT A - PRE-PROPOSAL INQUIRY (PPI) LOG.xlsx XLSX spreadsheet
ATTACHMENT D - HISTORICAL SMALL BUSINESS UTILIZATION.pdf PDF
Show all 35

On GovTribe

Work with this file

  • Download the original file
  • Contacts named in this file
  • Similar government files
  • Ask GovTribe AI about this file

Text version

DDG(X) LBTS WP3: E-Campus 1733372

SECTION 09 96 00

HIGH-PERFORMANCE COATINGS

11/14

PART 1 GENERAL

1.1 REFERENCES

The publications listed below form a part of this specification to the extent referenced. The publications are referred to within the text by the basic designation only.

MASTER PAINTERS INSTITUTE (MPI)

MPI ASM (2012) Architectural Painting Specification Manual

SOCIETY FOR PROTECTIVE COATINGS (SSPC)

SSPC 7/NACE No.4 (2007; E 2004) Brush-Off Blast Cleaning

1.2 SUBMITTALS

Government approval is required for submittals with a "G" designation;

submittals not having a "G" designation are for Contractor Quality Control approval. Submit the following in accordance with Section 01 33 00

SUBMITTAL PROCEDURES:

SD-01 Preconstruction Submittals

Equipment List; G

SD-03 Product Data

Epoxy Coatings; G

Polyurethane Coatings; G

SD-04 Samples

Color Chips; G

SD-07 Certificates

Epoxy Coatings; G

Polyurethane Coatings; G

Manufacturer's Printed Instructions; G

1.3 QUALITY CONTROL

Comply with Master Painters Institute (MPI) Standards indicated and listed in "MPI Approved Products List." Comply with the requirements in "MPI Architectural Painting Specification Manual" before any project is started.

Submit an equipment list consisting of a list of proposed equipment to be

SECTION 09 96 00 Page 1

June 17, 2025 used in performance of construction work.

Submit three color chips 3-inch by 4-inch or manufacture's pull-down of each finish color and gloss as scheduled.

1.4 DELIVERY, STORAGE, AND HANDLING

Deliver special coating materials to the project in their original containers bearing manufacturer's name, descriptive label, and coating formulations. Provide new and unopened containers.

Store special coating materials in tightly closed containers in a covered, well-ventilated area where they are not exposed to excessive heat, fumes, sparks, flame, or direct sunlight. Protect water-based coatings against freezing.

Store solvents, thinners, and equipment cleaners with the same care as the coating materials with ambient temperatures continuously maintained at a minimum 45 degrees F.

PART 2 PRODUCTS

2.1 PERFORMANCE REQUIREMENTS

Submit manufacturer's catalog data including manufacturer's name and identification. Include detailed data analysis of each special coating material required for the project, with all the coating constituents measured as percentages of the total weight of the coating. Also provide manufacturer's data concerning application, thinning, and average coverage per gallon

2.2 MATERIALS

2.2.1 Epoxy Coatings

Conform to MPI ASM, No. 116 for epoxy coatings and epoxy block filler, as modified.

Resins for finish coats are based on a polyamide-cured, epoxy-resin material. Apply finish coats with a dry-film thickness of not less than 4 mils per coat. Finish color and gloss are as indicated.

2.2.1.1 Ferrous and Galvanized Metal Surface Coatings

Coatings on ferrous and galvanized metal surfaces consist of a prime coat and not less than two finish coats. Comply with MPI ASM, No. 101 for an epoxy zinc primer with a metallic-zinc pigment for the substrate to be coated and the end use of the coated surface. Ensure resin solids and zinc pigment are not less than 80 percent of the total weight of the coating material. Apply prime coat with a total dry-film thickness of not less than 4 mils. Provide an epoxy-based finished coat as specified.

2.2.2 Polyurethane Coatings

Ensure polyurethane coatings conform to MPI ASM for each substrate indicated.

Resins for finish coats are based on a two-part, prepolymer, catalytic-cured, polyurethane material. Apply catalytic-cured coatings

SECTION 09 96 00 Page 2 with a total dry-film thickness of not less than 10 mils per coat.

Indicate finish color and gloss on the schedules.

2.2.2.1 Ferrous and Galvanized Metal Surface Coatings

Apply a polyurethane, pigmented coating system in conformance with MPI ASM, No. 72, MPI ASM, No. 77, and MPI ASM, No. 101 . Apply a prime coat with a dry-film thickness of not less than 2 mils. Finish coats are polyurethane-based material as specified.

2.2.3 Color

Color on exterior concrete walls must match Benjamin Moore paint color Red Rock, Number 2005-10. Submit color sample for review and approval.

For the cooling tower structure framing, submit the standard range of colors from the manufacturer for the Contracting Officer to select.

PART 3 EXECUTION

3.1 PREPARATION

3.1.1 Surface Preparation

Protect adjacent materials and equipment against damage from spillage, dripping, and spatter of coating materials. Leave clean building materials and equipment with all damaged surfaces corrected. Provide "WET PAINT" signs to indicate newly painted surfaces.

Protect work of other trades against damage from coating operation.

Correct damage by cleaning, repairing, replacing, and recoating, as approved by the Contracting Officer, and leave in an undamaged condition.

At completion of construction activities of other trades, touch up and restore damaged or defaced coated surfaces.

Provide forced ventilation for interior spaces during application and drying of coatings to prevent the buildup of toxic or explosive concentrations of solvent vapors.

Provide fire extinguishers of the required quantity and correct type to combat flammable liquid fires.

Dispose of rags that are used to wipe up coating materials, solvents, and thinners by drenching with water and placing them in a covered metal container

3.1.2 Cleaning

At end of each workday, remove rubbish, empty cans, rags, and other discarded materials from Project site.

After completing coating application, clean spattered surfaces. Remove spattered coatings by washing, scraping, or other methods. Do not scratch or damage adjacent finished surfaces.

Clean application equipment promptly and thoroughly with a suitable solvent after each use and stored in a clean, covered, well-ventilated container.

SECTION 09 96 00 Page 3

3.1.3 Concrete Surfaces

3.1.3.1 Steel Substrates

Remove rust and loose mill scale. Clean using methods recommended in writing by coating manufacturer. Conform to SSPC 7/NACE No.4 for blast cleaning.

3.1.3.2 Galvanized-Metal Substrates

Remove grease and oil residue from galvanized sheet metal fabricated from coil stock by mechanical methods to produce clean, lightly etched surfaces that promote adhesion of subsequently applied coatings.

3.1.4 Coating Material Preparation

Mix and prepare coating materials in accordance with the coating manufacturer's printed instructions for applying the particular material and coat. Keep materials which are not in actual use in closed containers.

Coating materials that have been mixed with an automatic shaker are allowed to stand to let air bubbles escape, then given a final hand mixing before application. Stir materials so as to produce a mixture of uniform density. Stir at frequent intervals during application to prevent skinning. Do not stir film which may form on the surface of the material. Remove film and strain, if necessary.

3.1.4.1 Thinning

Thinning is done in accordance with coating manufacturer's printed directions for the particular material and coat.

3.1.4.2 Tinting

Ensure prime and intermediate coats of paint are slightly different tints from the finish coat to facilitate identification of each coat. Tinting is done by the coating manufacturer and clearly identified as to color and coat.

3.2 APPLICATION

Do not perform exterior painting in damp or rainy weather. Interior painting is not allowed until the building is enclosed and has thoroughly dried out. Painting is not allowed below 50 degrees F or above 95 degrees F. Apply paint in accordance with the coating manufacturer's recommendations, and as specified.

Ensure coating application is done by skilled applicators. Apply coatings to clean and properly prepared surfaces. Apply coatings with clean, high-quality application equipment. Allow sufficient time between coats to ensure complete drying and curing. Sand and dust surfaces between coatings, as required, to produce a surface free of visible defects.

Lightly sand high gloss coatings and clear finishes between coats to ensure bond of following coats.

Apply coats to the surfaces in an even film. Cloudiness, spotting, holidays, laps, application marks, runs, sags, and other similar surface imperfections are not acceptable. Remove defective coating applications and re-coat as directed.

SECTION 09 96 00 Page 4

Ensure coating lines such as wainscots are sharp, true, and well-defined.

Tape may be used to establish coating lines, providing tape is removed before ragging or sawtooth edges form.

Ensure surfaces, including edges, corners, crevices, welds, and other similar changes in surface plane, meet the dry-film thickness not less than specified.

3.2.1 Brush Application

Use clean, proper size brushes for high-quality application of the specified coating materials. Brush out slow-dry coatings. Brush out quick-dry coatings only enough to spread out evenly.

3.2.2 Roller Application

Use clean roller covers of the proper nap length, nap texture, and material for high-quality application of the specified coating materials.

Ensure roller application is equivalent in all respects to the same coats applied by high-quality brush application.

3.2.3 Spray Application

Cover surfaces adjacent to sprayed areas to prevent damage from overspray, coating rebound, and spray drift.

3.3 FIELD QUALITY CONTROL

3.3.1 Field Test

Government may take dry-film tests from time to time on finished surfaces. Apply additional coatings to surfaces where there is less than the minimum specified dry-film thickness.

3.3.2 Repairing

Remove damaged and unacceptable portions of completed work and replace with new work to match adjacent surfaces at no additional cost to the Government.

-- End of Section --

SECTION 09 96 00 Page 5

THIS PAGE INTENTIONALLY LEFT BLANK

SECTION 09 96 00 Page 6

09 96 00 - HIGH-PERFORMANCE COATINGS
PART 1 GENERAL
1.1 REFERENCES
1.2 SUBMITTALS
1.3 QUALITY CONTROL
1.4 DELIVERY, STORAGE, AND HANDLING
PART 2 PRODUCTS
2.1 PERFORMANCE REQUIREMENTS
2.2 MATERIALS
2.2.1 Epoxy Coatings
2.2.1.1 Ferrous and Galvanized Metal Surface Coatings
2.2.2 Polyurethane Coatings
2.2.2.1 Ferrous and Galvanized Metal Surface Coatings

2.2.3 Color

PART 3 EXECUTION
3.1 PREPARATION
3.1.1 Surface Preparation
3.1.2 Cleaning
3.1.3 Concrete Surfaces
3.1.3.1 Steel Substrates
3.1.3.2 Galvanized-Metal Substrates
3.1.4 Coating Material Preparation
3.1.4.1 Thinning
3.1.4.2 Tinting
3.2 APPLICATION
3.2.1 Brush Application
3.2.2 Roller Application
3.2.3 Spray Application
3.3 FIELD QUALITY CONTROL
3.3.1 Field Test
3.3.2 Repairing

File details come from the government source that posted it. Updated .