5-C03 - Operations Facilities Expansion - Bid Specs - Vol I.pdf
PDF 6 MB Posted
- Attached to
- Oakbrook Center for Early Education
- Solicitation number
- US.252787
- Issued by
- Berks County, Reese CDP, Pennsylvania
About this file
This document is the Technical Specifications Volume I for the Operations Facilities Expansion project of the City of Lancaster Department of Public Works, located at 150 Pitney Road, Lancaster, Pennsylvania 17603, Project No. 25-061. The specifications detail construction requirements for Divisions 03 through 13, covering cast-in-place concrete, unit masonry, metals, wood composites, thermal and moisture protection, openings, finishes, specialties, furnishings, and special construction. The specifications establish comprehensive requirements for concrete materials, including cement type, aggregates, admixtures, and reinforcement; masonry units and mortar specifications; and associated finishing and quality control procedures. The document includes detailed sections on concrete mix design proportions for various applications (footings, interior slabs on metal deck, exterior slabs-on-grade), with compressive strength requirements ranging from 3,000 to 5,000 psi depending on application and exposure conditions. Administrative requirements mandate a preinstallation meeting one week before work begins, with extensive submittal requirements for product data, shop drawings, mix designs, material certificates, and qualification data for installers, concrete manufacturers, and testing agencies.
Quality assurance requirements specify that installers must be ACI-certified, concrete manufacturers must comply with ASTM C94 standards, and laboratory testing agencies must be qualified under ASTM C1077 with certified personnel. The specifications establish rigorous field quality control testing protocols including slump, air content, temperature, and compressive strength testing at prescribed frequencies, with acceptance criteria requiring that every average of three consecutive compressive strength tests equals or exceeds specified strength. Concrete curing requirements vary by application and surface type, with minimum durations of seven days for most applications and up to 28 days for certain floor treatments, employing methods such as moisture-retaining covers, water ponding, or membrane-forming curing compounds. Cold weather and hot weather concreting procedures are detailed with specific temperature thresholds and protection measures. Concrete finishing requirements include floor flatness and levelness tolerances per ASTM E1155, with F(F) and F(L) values specified for different surface types ranging from 20-35 and 15-25 respectively, measured within 48 hours of slab installation.
View the file
Other files
Show 40 more
Latest 50 of 63 listed here. See the rest on GovTribe.
On GovTribe
Work with this file
- Download the original file
- Contacts named in this file
- Similar government files
- Ask GovTribe AI about this file
Text version
250 Harrisburg Ave
Lancaster, PA 17603
OPERATIONS FACILITIES EXPANSION
CITY OF LANCASTER
DEPARTMENT OF PUBLIC WORKS
TECHNICAL SPECIFICATIONS
VOLUME I: DIVISIONS 03 - 13
OPERATIONS FACILITIES EXPANSION
150 PITNEY ROAD
LANCASTER, PA 17603
Project No. 25-061 September 8, 2026
Operations Facilities Expansion BH 25-061 City of Lancaster - Department of Public Works
TABLE OF CONTENTS 000110 - 1
SECTION 000110 - TABLE OF CONTENTS
VOLUME I
PROCUREMENT AND CONTRACTING REQUIREMENTS
SPECIFICATIONS
DIVISION 03 -- CONCRETE
033000 - CAST-IN-PLACE CONCRETE
DIVISION 04 -- MASONRY
042000 - UNIT MASONRY
DIVISION 05 -- METALS
051200 - STRUCTURAL STEEL FRAMING
052100 - STEEL JOIST FRAMING
053100 - STEEL DECKING
055000 - METAL FABRICATIONS
055100 - METAL STAIRS
055213 - PIPE AND TUBE RAILINGS
DIVISION 06 -- WOOD, PLASTICS, AND COMPOSITES
061000 - ROUGH CARPENTRY
061600 - SHEATHING
061753 - SHOP-FABRICATED WOOD TRUSSES
DIVISION 07 -- THERMAL AND MOISTURE PROTECTION
071113 - BITUMINOUS DAMPPROOFING
072100 - THERMAL INSULATION
072500 - WEATHER BARRIERS
077200 - ROOF ACCESSORIES
078400 - JOINT AND PENETRATION FIRESTOPPING
079200 - JOINT SEALANTS
DIVISION 08 -- OPENINGS
081113 - HOLLOW METAL DOORS AND FRAMES
083100 - ACCESS DOORS AND PANELS
083613 - SECTIONAL DOORS
084313 - ALUMINUM-FRAMED STOREFRONTS
087110 - DOOR HARDWARE
087111 - DOOR SCHEDULE
087112 - DOOR HARDWARE SCHEDULE
088000 - GLAZING
TABLE OF CONTENTS 000110 - 2
DIVISION 09 -- FINISHES
092116 - GYPSUM BOARD
092216 - NON-STRUCTURAL METAL FRAMING
093000 - CERAMIC TILING
095100 - ACOUSTICAL CEILINGS
096500 - RESILIENT FLOORING AND BASE
096710 - RESINOUS FLOORING
096813 - TILE CARPETING
099113 - EXTERIOR PAINTING
099123 - INTERIOR PAINTING
099723 - CONCRETE COATINGS
DIVISION 10 -- SPECIALTIES
101423 - PANEL SIGNAGE
102800 - TOILET, BATH, AND LAUNDRY ACCESSORIES
104400 - FIRE PROTECTION SPECIALTIES
105113 - METAL LOCKERS
105153 - LOCKER ROOM BENCHES
105629.16 - PALLET STORAGE RACKS
DIVISION 12 -- FURNISHINGS
122400 - WINDOW SHADES
123200 - MANUFACTURED WOOD CASEWORK
123600 - COUNTERTOPS
DIVISION 13 -- SPECIAL CONSTRUCTION
133419 - PRE-ENGINEERED METAL BUILDING SYSTEMS
VOLUME II
DIVISION 21 -- FIRE SUPPRESSION
210500 - COMMON WORK RESULTS FOR FIRE SUPPRESSION
210523 - GENERAL-DUTY VALVES FOR WATER-BASED FIRE-SUPPRESSION PIPING
210553 - IDENTIFICATION FOR FIRE SUPPRESSION PIPING AND EQUIPMENT
210719 - FIRE SUPPRESSION PIPING INSULATION
211300 - FIRE-SUPPRESSION SPRINKLER SYSTEMS
DIVISION 22 -- PLUMBING
220513 - COMMON MOTOR REQUIREMENTS FOR PLUMBING EQUIPMENT
220517 - SLEEVES AND SLEEVE SEALS FOR PLUMBING PIPING
220519 - METERS AND GAUGES FOR PLUMBING PIPING
220523 - GENERAL-DUTY VALVES FOR PLUMBING PIPING
220529 - HANGERS AND SUPPORTS FOR PLUMBING PIPING AND EQUIPMENT
220553 - IDENTIFICATION FOR PLUMBING PIPING AND EQUIPMENT
220719 - PLUMBING PIPING INSULATION
221005 - PLUMBING PIPING
TABLE OF CONTENTS 000110 - 3
221119 - DOMESTIC WATER PIPING SPECIALTIES
221123 - DOMESTIC WATER PUMPS
221319 - SANITARY WASTE PIPING SPECIALTIES
223323 - SANITARY WASTE INTERCEPTORS
223000 - PLUMBING EQUIPMENT
224000 - PLUMBING FIXTURES
DIVISION 23 -- HEATING, VENTILATING, AND AIR-CONDITIONING (HVAC)
230130.51 - HVAC AIR-DISTRIBUTION SYSTEM CLEANING
230513 - COMMON MOTOR REQUIREMENTS FOR HVAC EQUIPMENT
230529 - HANGERS AND SUPPORTS FOR HVAC PIPING AND EQUIPMENT
230548 - VIBRATION AND SEISMIC CONTROLS FOR HVAC - MASON
230553 - IDENTIFICATION FOR HVAC PIPING AND EQUIPMENT
230593 - TESTING, ADJUSTING, AND BALANCING FOR HVAC
230713 - DUCT INSULATION
230913 - INSTRUMENTATION AND CONTROL DEVICES FOR HVAC
232300 - REFRIGERANT PIPING
233100 - HVAC DUCTS AND CASINGS
233300 - AIR DUCT ACCESSORIES
233416 - CENTRIFUGAL HVAC FANS
233439 - HIGH-VOLUME, LOW-SPEED PROPELLER FANS
233700 - AIR OUTLETS AND INLETS
235533 - FUEL-FIRED UNIT HEATERS
238126.13 - SMALL-CAPACITY SPLIT-SYSTEM AIR CONDITIONERS
DIVISION 26 -- ELECTRICAL
260519 - LOW-VOLTAGE ELECTRICAL POWER CONDUCTORS AND CABLES
260526 - GROUNDING AND BONDING FOR ELECTRICAL SYSTEMS
260529 - HANGERS AND SUPPORTS FOR ELECTRICAL SYSTEMS
260533.13 - CONDUIT FOR ELECTRICAL SYSTEMS
260533.16 - BOXES FOR ELECTRICAL SYSTEMS
260533.23 - SURFACE RACEWAYS FOR ELECTRICAL SYSTEMS
260553 - IDENTIFICATION FOR ELECTRICAL SYSTEMS
260923 - LIGHTING CONTROL DEVICES
262100 - LOW-VOLTAGE ELECTRICAL SERVICE ENTRANCE
262416 - PANELBOARDS
262726 - WIRING DEVICES
262816.13 - ENCLOSED CIRCUIT BREAKERS
262816.16 - ENCLOSED SWITCHES
263213 - ENGINE GENERATORS
263600 - TRANSFER SWITCHES
265100 - INTERIOR LIGHTING
265600 - EXTERIOR LIGHTING
DIVISION 27 -- COMMUNICATIONS
270529 - HANGERS AND SUPPORTS FOR COMMUNICATIONS SYSTEMS
270533.13 - CONDUIT FOR COMMUNICATIONS SYSTEMS
271000 - STRUCTURED CABLING
TABLE OF CONTENTS 000110 - 4
DIVISION 28 -- ELECTRONIC SAFETY AND SECURITY
281000 - ACCESS CONTROL
284600 - FIRE DETECTION AND ALARM
CAST-IN-PLACE CONCRETE 033000 - 1
SECTION 033000 - CAST-IN-PLACE CONCRETE
PART 1 GENERAL
1.1 SECTION INCLUDES
A. Cast-in-place concrete, including concrete materials, mixture design, and finishes.
B. Concrete formwork.
C. Concrete foundations and anchor bolts for pre-engineered building.
D. Concrete reinforcement.
E. Joint devices associated with concrete work.
F. Concrete curing.
1.2 RELATED REQUIREMENTS
A. Section 079200 - Joint Sealants: Products and installation for sealants and joint fillers for saw cut joints and isolation joints in slabs.
B. See Site Specifications for concrete paving, walks and curbs.
1.3 DEFINITIONS
A. Cementitious Materials: Portland cement, including in combination with one or more of the following: blended hydraulic cement, fly ash, slag cement, other pozzolans, and silica fume;
materials subject to compliance with requirements.
B. Water/Cement Ratio (w/cm): The ratio by weight of water to cementitious materials
1.4 REFERENCE STANDARDS
A. ACI CODE-318 - Building Code for Structural Concrete—Code Requirements and Commentary; 2025.
B. ACI PRC-211.1 - Selecting Proportions for Normal-Density and High Density-Concrete - Guide; 2022.
C. ACI PRC-302.1 - Guide to Concrete Floor and Slab Construction; 2015.
D. ACI PRC-304 - Guide for Measuring, Mixing, Transporting, and Placing Concrete; 2000 (Reapproved 2009).
E. ACI PRC-305 - Guide to Hot Weather Concreting; 2020.
F. ACI PRC-306 - Guide to Cold Weather Concreting; 2016.
CAST-IN-PLACE CONCRETE 033000 - 2
G. ACI PRC-308 - Guide to External Curing of Concrete; 2016.
H. ACI SPEC-301 - Specifications for Concrete Construction; 2020.
I. AISC 303 - Code of Standard Practice for Steel Buildings and Bridges; 2022, with Errata (2025).
J. ASTM C31/C31M - Standard Practice for Making and Curing Concrete Test Specimens in the Field; 2024.
K. ASTM C33/C33M - Standard Specification for Concrete Aggregates; 2024a.
L. ASTM C39/C39M - Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens; 2026.
M. ASTM C94/C94M - Standard Specification for Ready-Mixed Concrete; 2026a.
N. ASTM C143/C143M - Standard Test Method for Slump of Concrete; 2026a.
O. ASTM C150/C150M - Standard Specification for Portland Cement; 2022.
P. ASTM C171 - Standard Specification for Sheet Materials for Curing Concrete; 2020.
Q. ASTM C172/C172M - Standard Practice for Sampling Freshly Mixed Concrete; 2017.
R. ASTM C260/C260M - Standard Specification for Air-Entraining Admixtures for Concrete;
2010a (Reapproved 2016).
S. ASTM C309 - Standard Specification for Liquid Membrane-Forming Compounds for Curing Concrete; 2025.
T. ASTM C494/C494M - Standard Specification for Chemical Admixtures for Concrete; 2024.
U. ASTM C618 - Standard Specification for Coal Ash and Raw or Calcined Natural Pozzolan for Use in Concrete; 2025a.
V. ASTM C685/C685M - Standard Specification for Concrete Made by Volumetric Batching and Continuous Mixing; 2025a.
W. ASTM C881/C881M - Standard Specification for Epoxy-Resin-Base Bonding Systems for Concrete; 2020a.
X. ASTM C989/C989M - Standard Specification for Slag Cement for Use in Concrete and Mortars; 2025.
Y. ASTM C1077 - Standard Practice for Agencies Testing Concrete and Concrete Aggregates for Use in Construction and Criteria for Testing Agency Evaluation; 2024.
Z. ASTM C1116/C1116M - Standard Specification for Fiber-Reinforced Concrete; 2023.
AA. ASTM C1315 - Standard Specification for Liquid Membrane-Forming Compounds Having Special Properties for Curing and Sealing Concrete; 2025.
CAST-IN-PLACE CONCRETE 033000 - 3
BB. ASTM C1602/C1602M - Standard Specification for Mixing Water Used in the Production of Hydraulic Cement Concrete; 2022.
CC. ASTM D1751 - Standard Specification for Preformed Expansion Joint Filler for Concrete Paving and Structural Construction (Nonextruding and Resilient Asphalt Types); 2023.
DD. ASTM D2240 - Standard Test Method for Rubber Property--Durometer Hardness; 2015 (Reapproved 2021).
EE. ASTM D3963/D3963M - Standard Specification for Fabrication and Jobsite Handling of Epoxy-Coated Steel Reinforcing Bars; 2021.
FF. ASTM E329 - Standard Specification for Agencies Engaged in Construction Inspection, Testing, or Special Inspection; 2023.
GG. ASTM E1155/E1155M - Standard Test Method for Determining FF Floor Flatness and FL Floor Levelness Numbers; 2023.
HH. ASTM E1643 - Standard Practice for Selection, Design, Installation, and Inspection of Water Vapor Retarders Used in Contact with Earth or Granular Fill Under Concrete Slabs; 2024.
II. ASTM E1745 - Standard Specification for Plastic Water Vapor Retarders Used in Contact with Soil or Granular Fill under Concrete Slabs; 2017 (Reapproved 2023).
JJ. COE CRD-C 48 - Handbook for Concrete and Cement Standard Test Method for Water Permeability of Concrete; 1992.
1.5 ADMINISTRATIVE REQUIREMENTS
A. Preinstallation Meeting: Conduct a preinstallation meeting one week before starting work of this section; require attendance by all affected installers.
1. Review the following:
a. Special inspection and testing and inspecting agency procedures for field quality control.
b. Construction joints, control joints, isolation joints, and joint-filler strips.
c. Semirigid joint fillers.
d. Vapor-retarder installation.
e. Anchor rod and anchorage device installation tolerances.
f. Cold and hot weather concreting procedures.
g. Concrete finishes and finishing.
h. Curing procedures.
i. Forms and form-removal limitations.
j. Concrete repair procedures.
k. Concrete protection.
l. Initial curing and field curing of field test cylinders (ASTM C31/C31M.)
m. Protection of field cured field test cylinders.
CAST-IN-PLACE CONCRETE 033000 - 4
1.6 SUBMITTALS
A. Product Data: Submit manufacturers' data on manufactured products showing compliance with specified requirements and installation instructions. Include the following:
1. Include the following:
a. Portland cement.
b. Fly ash.
c. Slag cement.
d. Aggregates.
e. Admixtures:
1) Include limitations of use, including restrictions on cementitious materials, supplementary cementitious materials, air entrainment, aggregates, temperature at time of concrete placement, relative humidity at time of concrete placement, curing conditions, and use of other admixtures.
f. Fiber reinforcement.
g. Vapor retarders.
h. Curing materials.
1) For curing compounds, provide data on method of removal in the event of incompatibility with floor covering adhesives.
2) Include documentation from color pigment manufacturer, indicating that proposed methods of curing are recommended by color pigment manufacturer.
i. Joint fillers.
j. Repair materials.
B. Mix Design: Submit proposed concrete mix design.
1. Include the following:
a. Mixture identification.
b. Minimum 28-day compressive strength.
c. Durability exposure class.
d. Maximum w/cm.
e. Slump limit.
f. Air content.
g. Nominal maximum aggregate size.
h. Intended placement method.
i. Indicate amounts of mixing water to be withheld for later addition at Project site if permitted.
j. Submit alternate design mixtures when characteristics of materials, Project conditions, weather, test results, or other circumstances warrant adjustments.
C. Shop Drawings:
1. Construction Joint Layout: Indicate proposed construction joints required to construct the structure.
a. Location of construction joints is subject to approval of the Architect.
2. Steel Reinforcement Shop Drawings: Placing drawings that detail fabrication, bending, and placement. Include bar sizes, lengths, material, grade, bar schedules, stirrup spacing, bent bar diagrams, bar arrangement, splices and laps, mechanical connections, tie spacing, hoop spacing, and supports for concrete reinforcement.
CAST-IN-PLACE CONCRETE 033000 - 5
3. Design Mixes: For each concrete mix. Include alternate mix designs when characteristics of materials, project conditions, weather, test results, or other circumstances warrant adjustments.
a. If mix water is to be withheld at the plant and later added at the Project site to provide the water to cement ratio of the design mix, this must be clearly indicated on EVERY delivery ticket to the Project site.
D. Qualification Data:
1. Installer: Include copies of applicable ACI certificates.
2. Ready-mixed concrete manufacturer.
3. Testing agency: Include copies of applicable ACI certificates.
E. Material Certificates: For each of the following, signed by manufacturers:
1. Cementitious materials.
2. Admixtures.
3. Fiber reinforcement.
4. Curing compounds.
5. Floor and slab treatments.
6. Bonding agents.
7. Adhesives.
8. Vapor retarders.
9. Semirigid joint filler.
10. Joint-filler strips.
11. Repair materials.
F. Material Test Reports: Submit report for each test or series of tests specified.
1. Portland cement.
2. Fly ash.
3. Slag cement.
4. Performance-based hydraulic cement.
5. Aggregates.
6. Admixtures:
a. Permeability-Reducing Admixture: Include independent test reports, indicating compliance with specified requirements, including dosage rate used in test.
G. Preconstruction Test Reports: For each mix design.
H. Field quality-control reports.
I. Minutes of preinstallation conference.
1.7 QUALITY ASSURANCE
A. Installer Qualifications: A qualified installer who employs Project personnel qualified as an ACI-certified Flatwork Technician and Finisher and a supervisor who is a certified ACI Flatwork Concrete Finisher/Technician or an ACI Concrete Flatwork Technician.
CAST-IN-PLACE CONCRETE 033000 - 6
1. Post-Installed Concrete Anchors Installers: ACI-certified Adhesive Anchor Installer.
B. Ready-Mixed Concrete Manufacturer Qualifications: A firm experienced in manufacturing ready-mixed concrete products and that complies with ASTM C94/C94M requirements for production facilities and equipment.
1. Manufacturer certified in accordance with NRMCA's "Certification of Ready Mixed Concrete Production Facilities."
C. Laboratory Testing Agency Qualifications: A testing agency qualified in accordance with ASTM C1077 and ASTM E329 for testing indicated and employing an ACI-certified Concrete Quality Control Technical Manager.
1. Personnel performing laboratory tests shall be an ACI-certified Concrete Strength Testing Technician and Concrete Laboratory Testing Technician, Grade I. Testing agency laboratory supervisor shall be an ACI-certified Concrete Laboratory Testing Technician, Grade II.
D. Field Quality Control Testing Agency Qualifications: An independent agency, acceptable to authorities having jurisdiction, qualified in accordance with ASTM C1077 and ASTM E329 for testing indicated.
1. Personnel conducting field tests shall be qualified as an ACI Concrete Field Testing Technician, Grade 1, in accordance with ACI CPP 610.1 or an equivalent certification program.
E. Perform work of this section in accordance with ACI SPEC-301 and ACI CODE-318.
F. Follow recommendations of ACI PRC-305 when concreting during hot weather, and as follows:
1. Maintain concrete temperature at time of discharge to not exceed 95 deg F (35 deg C).
2. Fog-spray forms, steel reinforcement, and subgrade just before placing concrete. Keep subgrade uniformly moist without standing water, soft spots, or dry areas.
G. Follow recommendations of ACI PRC-306 when concreting during cold weather, and as follows:
1. Protect concrete work from physical damage or reduced strength that could be caused by frost, freezing actions, or low temperatures.
2. When average high and low temperature is expected to fall below 40 deg F (4.4 deg C) for three successive days, maintain delivered concrete mixture temperature within the temperature range required by ACI 301 (ACI 301M).
3. Do not use frozen materials or materials containing ice or snow.
4. Do not place concrete in contact with surfaces less than 35 deg F (1.7 deg C), other than reinforcing steel.
5. Do not use calcium chloride, salt, or other materials containing antifreeze agents or chemical accelerators unless otherwise specified and approved in mixture designs.
CAST-IN-PLACE CONCRETE 033000 - 7
1.8 PRECONSTRUCTION TESTING
A. Preconstruction Testing Service: Engage a qualified testing agency to perform preconstruction testing on each concrete mixture.
1. Include the following information in each test report:
a. Admixture dosage rates.
b. Slump.
c. Air content.
d. Seven-day compressive strength.
e. 28-day compressive strength.
f. Permeability.
1.9 DELIVERY, STORAGE AND HANDLING
A. Comply with ASTM C94/C94M and ACI 301 (ACI 301M).
1.10 WARRANTY
A. See Section 017800 - Closeout Submittals for additional warranty requirements.
PART 2 PRODUCTS
2.1 FORMWORK
A. Form Materials: Contractor's choice of standard products with sufficient strength to withstand hydrostatic head without distortion in excess of permitted tolerances.
1. Form Coating: Release agent that will not adversely affect concrete or interfere with application of coatings.
2. Form Ties: Cone snap type that will leave no metal within 1-1/2 inches (38 mm) of concrete surface.
2.2 CONCRETE MATERIALS
A. General: Comply with ACI 301 (ACI 301M)
B. Source Limitations:
1. Obtain all concrete mixtures from a single ready-mixed concrete manufacturer for entire Project.
2. Obtain each type or class of cementitious material of the same brand from the same manufacturer's plant.
3. Obtain aggregate from single source.
4. Obtain each type of admixture from single source from single manufacturer.
C. Cement: ASTM C150/C150M, Type I - Normal Portland type.
CAST-IN-PLACE CONCRETE 033000 - 8
D. Normal-Weight Aggregates: ASTM C33/C33M, coarse aggregate or better; graded.
1. Acquire aggregates for entire project from same source.
2. Alkali-Silica Reaction: Comply with one of the following:
a. Expansion Result of Aggregate: Not more than 0.04 percent at one-year when tested in accordance with ASTM C1293.
b. Expansion Results of Aggregate and Cementitious Materials in Combination: Not more than 0.10 percent at an age of 16 days when tested in accordance with ASTM C1567.
c. Alkali Content in Concrete: Not more than 4 lb./cu. yd. (2.37 kg/cu. m) for moderately reactive aggregate or 3 lb./cu. yd. (1.78 kg/cu. m) for highly reactive aggregate, when tested in accordance with ASTM C1293 and categorized in accordance with ASTM C1778, based on alkali content being calculated in accordance with ACI 301 (ACI 301M).
3. Fine Aggregate: Free of materials with deleterious reactivity to alkali in cement.
E. Fly Ash: ASTM C618, Class C or F.
F. Ground Granulated Blast Furnace Slag: ASTM C989/C989M, Grade 100 or 120.
G. Water: ASTM C1602/C1602M; clean, potable, and not detrimental to concrete.
2.3 ADMIXTURES
A. Do not use chemicals that will result in soluble chloride ions in excess of 0.1 percent by weight of cement. Do not use calcium chloride or admixtures containing calcium chloride.
B. Air Entrainment Admixture: ASTM C260/C260M.
C. High Range Water Reducing Admixture: ASTM C494/C494M Type F.
D. Water Reducing Admixture: ASTM C494/C494M Type A.
E. Water Reducing and Retarding Admixture: ASTM C494/C494M Type D.
F. Retarding Admixture: ASTM C494/C494M Type B.
G. Set-Accelerating, Corrosion Inhibiting Admixture: Commercially formulated, anodic inhibitor or mixed cathodic and anodic inhibitor; capable of forming a protective barrier and minimizing chloride reactions with steel reinforcement in concrete.
1. ASTM C494/C494M, Type C.
2. Products: Subject to compliance with requirements, available products that may be incorporated into the Work include, but are not limited to, the following:
a. BASF Construction Chemicals - Building Systems; Rheocrete CNI:
https://construction.basf.com/global/en/#sle.
b. Euclid Chemical Company; EUCON CIA: www.euclidchemical.com/#sle.
c. GCP Applied Technologies; DCI: www.gcpat.com/#sle.
d. Sika Corporation; Sika CNI: usa.sika.com/#sle.
CAST-IN-PLACE CONCRETE 033000 - 9
H. Non-Set-Accelerating Corrosion-Inhibiting Admixture: Commercially formulated, non-set-accelerating, anodic inhibitor, or mixed cathodic and anodic inhibitor; capable of forming a protective barrier and minimizing chloride reactions with steel reinforcement in concrete.
1. Products: Subject to compliance with requirements, available products that may be incorporated into the Work include, but are not limited to, the following:
a. BASF Construction Chemicals - Building Systems; Rheocrete 222+:
https://construction.basf.com/global/en/#sle.
b. Cortec Corporation: MCI-2000/2005NS: www.cortecvci.com/#sle.
c. GCP Applied Technologies; DCI-S: www.gcpat.com/#sle.
d. Sika Corporation; FerroGard 901: usa.sika.com/#sle.
I. Waterproofing Admixture: Admixture formulated to reduce permeability to liquid water, with no adverse effect on concrete properties.
1. Admixture Composition: Crystalline, functioning by growth of crystals in capillary pores.
2. Admixture Composition: Hydrophobic polymer waterproofing and corrosion inhibitor, functioning by closing concrete pores and chemical bonding.
3. Permeability of Cured Concrete: No measurable leakage when tested in accordance with
COE CRD-C 48 at 200 psi (1.38 MPa); provide test reports.
4. Products:
a. Aquafin, Inc: www.aquafin.net/#sle.
b. Barrier One Concrete Admixtures; WPX Water Proofer: www.barrierone.com/#sle.
c. ConShield Technologies, Inc: www.conshield.com/#sle.
d. Euclid Chemical Company; Eucon Vandex AM-10: www.euclidchemical.com/#sle.
e. Fullforce by ABC Polymers Industries, LLC; DuraForce (iwp):
www.fullforcesolutions.us/#sle.
f. Hycrete, Inc: www.hycrete.com/#sle.
g. ISE Logik Industries, Inc; DuraForce(i): www.iselogik.com/#sle.
h. Kryton International, Inc; Krystol Internal Membrane (KIM): www.kryton.com/#sle.
i. Master Builders Solutions; MasterLife 300: www.master-builders-solutions.com/en-us/#sle.
j. Penetron; PENETRON ADMIX SB: www.penetron.com/#sle.
k. Specialty Products Group; Vapor Lock 20/21: www.spggogreen.com/#sle.
l. W. R. Meadows, Inc; ADI-CON CW Plus: www.wrmeadows.com/#sle.
J. Water and Water Used to Make Ice: ASTM C94/C94M, potable.
2.4 ACCESSORY MATERIALS
A. Underslab Vapor Retarder:
1. Sheet Material: ASTM E1745, Class A; stated by manufacturer as suitable for installation in contact with soil or granular fill under concrete slabs. Single-ply polyethylene is prohibited.
2. Accessory Products: Vapor retarder manufacturer's recommended tape, adhesive, mastic, prefabricated boots, etc., for sealing seams and penetrations.
3. Products: Subject to compliance with requirements, provide one of the following:
a. Barrier-Bac, Inc.; VB-350 16 mil Class A Vapor Retarder: www.barrierbac.com/#sle.
CAST-IN-PLACE CONCRETE 033000 - 10
b. ISI Building Products; Viper VaporCheck II 15-mil (Class A): www.isibp.com/#sle.
c. Stego Industries, LLC; Stego Wrap 15-mil Class A Vapor Barrier:
www.stegoindustries.com/#sle.
d. Tex-Trude, LP; Xtreme Vapor Barrier (20-mil): www.tex-trude.com/#sle.
2.5 BONDING AND JOINTING PRODUCTS
A. Epoxy Bonding System:
1. Complying with ASTM C881/C881M and of Type required for specific application.
2. Capable of humid curing and bonding to damp surfaces, of class suitable for application temperature and of grade and class to suit requirements, and as follows:
a. Types IV and V, load bearing, for bonding hardened or freshly mixed concrete to hardened concrete.
B. Slab Isolation Joint Filler: 1/2-inch (13 mm) thick, height equal to slab thickness, with removable top section forming 1/2-inch (13 mm) deep sealant pocket after removal.
1. Material: ASTM D1751, cellulose fiber.
C. Semirigid Joint Filler: Two-component, semirigid, 100 percent solids, in accordance with
ASTM D2240.
2.6 CURING MATERIALS
A. Evaporation Reducer: Liquid thin-film-forming compound that reduces rapid moisture loss caused by high temperature, low humidity, and high winds; intended for application immediately after concrete placement.
1. Products:
a. ChemMasters, Inc.; Spray Film: www.chemmasters.net/#sle.
b. Dayton Superior Corporation; Sure Film: www.daytonsuperior.com/#sle.
c. Euclid Chemical Company ; EUCOBAR: www.euclidchemical.com/#sle.
d. Kaufman Products Inc; VaporAid: www.kaufmanproducts.net/#sle.
e. Lambert Corporation; Lambco Skin: https://www.lambertusa.net/#sle.
f. Laticrete International, Inc.; L&M E-CON: www.laticrete.com/#sle.
g. Master Builders Solutions; MasterKure ER 50: www.master-builders-solutions.com/en-us/#sle.
h. Metalcrete Industries; Waterhold: metalcreteindustries.com/#sle.
i. Sika Corporation; SikaFilm: usa.sika.com/#sle.
j. SpecChem, LLC; SpecFilm Concentrate or SpecFilm: www.specchemllc.com/#sle.
k. W. R. Meadows, Inc; Evapre or Evapre-RTU: www.wrmeadows.com/#sle.
B. Absorptive Cover: AASHTO M 182, Class 2, burlap cloth made from jute or kenaf, weighing approximately 9 oz./sq. yd. (305 g/sq. m) when dry.
C. Moisture-Retaining Cover: ASTM C171, polyethylene film burlap-polyethylene sheet.
1. Color:
a. Ambient Temperature Below 50 deg F (10 deg C): Black.
CAST-IN-PLACE CONCRETE 033000 - 11
b. Ambient Temperature between 50 deg F (10 deg C) and 85 deg F (29 deg C): Any color.
2. Ambient Temperature Above 85 deg F (29 deg C): White.
D. Curing Compound, Hardener, and Dustproofer for Exposed, Sealed Concrete Areas:
Liquid, membrane-forming, clear, water-based curing agent; complying with ASTM C309, Type 1, Class A, formulated to perform with products specified in Section 099723 - Concrete Coatings.
1. Vehicle: Water-based.
2. Basis-of-Design Product: Provide MED-CURE Concrete Curing Agent as manufactured by W.R. Meadows, Inc., or equal as approved by the Architect in writing before the Bid.
a. Approved Equals: Product approved by approved manufacturer under Section 099723
- Concrete Coatings.
E. Curing Compound, Non-Dissipating: Liquid, membrane-forming, clear, nonyellowing acrylic;
complying with ASTM C309, Type 1, Class B, 18 to 25 percent solids, nondissipating, certified by curing compound manufacturer to not interfere with bonding of floor covering.
1. Vehicle: Water-based.
2. Products:
a. ChemMasters, Inc.; Safe-Cure & Seal 309: https://www.chemmasters.net/#sle.
b. Cresset Chemical Company; Crete-Trete 309-VOC Cure & Seal:
c. Dayton Superior Corporation; Cure & Seal 309 J18: www.daytonsuperior.com/#sle.
d. Euclid Chemical Company; AQUA-CURE VOX: www.euclidchemical.com/#sle.
e. Kaufman Products Inc; Krystal 15 Emulsion: www.kaufmanproducts.net/#sle.
f. Lambert Corporation; Crystal Clear Seal WB: www.lambertusa.net/#sle.
g. LATICRETE International, Inc; Dress & Seal WB: www.laticrete.com/#sle.
h. Metalcrete Industries; Metcure: metalcreteindustries.com/#sle.
i. Nox-Crete Inc; Cure & Seal 150E: www.nox-crete.com/#sle.
j. W. R. Meadows, Inc; VOCOMP-20: www.wrmeadows.com/#sle.
F. Curing and Sealing Compound, Low Gloss: Liquid, membrane-forming, clear, non-yellowing acrylic; complying with ASTM C1315 Type 1 Class A.
1. Products:
a. ChemMasters, Inc.; Polyseal WB: https://www.chemmasters.net/#sle.
b. Lambert Corporation; Crystal Clear Seal 1315 WB: www.lambertusa.net/#sle.
c. Metalcrete Industries; Metcure 30: metalcreteindustries.com/#sle.
d. W. R. Meadows, Inc; VOCOMP-30: www.wrmeadows.com/#sle.
G. Water: Potable, not detrimental to concrete.
2.7 CONCRETE MIX DESIGN
A. Proportioning Normal Weight Concrete: Comply with ACI PRC-211.1 recommendations.
1. Under circumstances where laboratory trial mix or field test data are not available, the required average compressive strength of concrete produced with materials similar to those specified shall be at least 1,200 psi greater than the specified compressive
CAST-IN-PLACE CONCRETE 033000 - 12
strength. This alternative shall not be permitted if the specified compressive strength is greater than 4,000 psi.
B. Use a qualified independent testing agency for preparing and reporting proposed mix designs for the laboratory trial mix basis.
C. Air Content: Add air-entraining admixture at manufacturer's prescribed rate to result in concrete at point of placement having an air content as follows within a tolerance of plus 1 or minus 1.5 percent, unless otherwise indicated:
1. Air Content: 6 percent for 3/4-inch nominal maximum aggregate size.
D. Do not air entrain concrete to trowel-finished interior floors and suspended slabs. Do not allow entrapped air content to exceed 3 percent.
E. Limit water-soluble, chloride-ion content in hardened concrete to 0.15 percent by weight of cement.
F. Admixtures: Add acceptable admixtures as recommended in ACI PRC-211.1 and at rates recommended or required by manufacturer.
1. Use admixtures according to manufacturer's written instructions.
2. Use water-reducing admixture or high-range water-reducing admixture (superplasticizer) in concrete, as required, for placement and workability.
3. Use water-reducing and retarding admixture when required by high temperatures, low humidity, or other adverse placement conditions.
G. Piers, and Foundation/Retaining Walls: Proportion normal-weight concrete mix as follows:
1. Compressive Strength, when tested in accordance with ASTM C39/C39M at 28 days:
4,000 pounds per square inch (27.6 MPa), except 4,500 psi where exposed to moisture and freeze-thaw condition
2. Fly Ash Content: Maximum 18 percent of cementitious materials by weight.
3. Ground Granulated Blast-Furnace Slag Content: Maximum 50 percent of cementitious materials by weight.
4. Water-Cement Ratio: Maximum 50 percent by weight.
5. Maximum Slump: 4 inches (100 mm).
6. Maximum Slump for Concrete Containing High-Range Water-Reducing Admixture: 8 inches after admixture is added to concrete with 2-to-4-inch slump.
H. Footings: Proportion normal-weight concrete mix as follows:
1. Compressive Strength, when tested in accordance with ASTM C39/C39M at 28 days:
3,000 pounds per square inch (20.7 MPa), except 4,500 psi where exposed to moisture and freeze-thaw condition
2. Fly Ash Content: Maximum 18 percent of cementitious materials by weight.
3. Ground Granulated Blast-Furnace Slag Content: Maximum 50 percent of cementitious materials by weight.
4. Water-Cement Ratio: Maximum 50 percent by weight.
5. Maximum Slump: 4 inches (100 mm).
CAST-IN-PLACE CONCRETE 033000 - 13
6. Maximum Slump for Concrete Containing High-Range Water-Reducing Admixture: 8 inches after admixture is added to concrete with 2-to-4-inch slump.
7. Maximum Aggregate Size: 5/8 inch (16 mm).
I. Interior Slabs-on-Metal Deck: Proportion normal-weight concrete mix as follows:
1. Compressive Strength, when tested in accordance with ASTM C39/C39M at 28 days:
3,500 pounds per square inch (24.1 MPa).
2. Minimum Cementitious Materials Content: 520 lb./cu. yd.
3. Fly Ash Content: Maximum 18 percent of cementitious materials by weight.
4. Ground Granulated Blast-Furnace Slag Content: Maximum 50 percent of cementitious materials by weight.
5. Water-Cement Ratio: Maximum 47 percent by weight.
a. Interior slab mix is to contain a high-range, water-reducing admixture.
6. Maximum Slump: Produce a mix that has the minimum amount of water necessary to generate a 2-to-3-inch slump prior to the addition of any water reducing admixtures, as recommended in ACI 302.1R, “Concrete Floor and Slab Construction”, Chapter 6, “Concrete Properties and Consistency”.
7. Maximum Slump for Concrete Containing High-Range Water-Reducing Admixture: 8 inches after admixture is added to concrete.
J. Exterior Slabs-on-Grade: Proportion normal-weight concrete mix as follows:
1. Compressive Strength, when tested in accordance with ASTM C39/C39M at 28 days:
4,500 pounds per square inch (31 MPa).
2. Minimum Cementitious Materials Content: 520 lb./cu. yd.
3. Fly Ash Content: Maximum 18 percent of cementitious materials by weight.
4. Ground Granulated Blast-Furnace Slag Content: Maximum 50 percent of cementitious materials by weight.
5. Water-Cement Ratio: Maximum 45 percent by weight.
a. Interior slab mix is to contain a high-range, water-reducing admixture.
6. Maximum Slump: Produce a mix that has the minimum amount of water necessary to generate a 4-inch maximum slump prior to the addition of any water reducing admixtures, as recommended in ACI 302.1R, “Concrete Floor and Slab Construction”, Chapter 6, “Concrete Properties and Consistency”.
7. Provide air-entrainment admixture.
K. Concrete Mixtures for Site Elements
1. Class A: Normal-weight concrete used for footings, walk-off pads, grade beams, and tie beams.
2. Compressive Strength, when tested in accordance with ASTM C39/C39M at 28 days:
5,000 pounds per square inch (34.5 MPa).
3. Fly Ash Content: Maximum 25 percent of cementitious materials by weight.
4. Silica Fume Content: Maximum 10 percent of cementitious materials by weight.
5. Water-Cement Ratio: Maximum 45 percent by weight.
a. Interior slab mix is to contain a high-range, water-reducing admixture.
6. Maximum Slump: 4 inches, plus or minus 1 inch.
7. Slump Flow Limit: 22 inches, plus or minus 1.5 inches.
8. Air Content:
CAST-IN-PLACE CONCRETE 033000 - 14
a. Exposure Classes F2 and F3: 5.5 percent, plus or minus 1.5 percent at point of delivery for concrete containing 1-1/2-inch nominal maximum aggregate size.
2.8 FABRICATING REINFORCEMENT
A. Fabricate steel reinforcement according to CRSI's "Manual of Standard Practice”.
2.9 MIXING
A. Ready-Mixed Concrete: Measure, batch, mix, and deliver concrete according to ASTM C94/C94M and ASTM C1116/C1116M and furnish batch ticket information for EACH delivery to the Project site.
1. When air temperature is between 85 and 90 deg. F, reduce mixing and delivery time from 1-1/2 hours to 75 minutes; when air temperature is above 90 deg F, reduce mixing and delivery time to 60 minutes.
B. On Project Site: Mix in drum type batch mixer, complying with ASTM C685/C685M.
1. For mixer capacity of 1 cu. yd., or smaller, mix each batch not less than 1-1/2 minutes and not more than 5 minutes.
2. For mixer capacity larger than 1 cu. yd., increase mixing time by 15 seconds for each additional 1 cu. yd.
3. Provide batch ticket for each batch discharged and used in the Work, indicating Project identification name and number, date, mixture type, mixture time, quantity, and amount of water added. Record approximate location of final deposit in structure.
C. Transit Mixers: Comply with ASTM C94/C94M.
D. Adding Water: If concrete arrives on-site with slump less than suitable for placement, do not add water that exceeds the maximum water-cement ratio or exceeds the maximum permissible slump.
PART 3 EXECUTION
3.1 EXAMINATION
A. Verify lines, levels, and dimensions before proceeding with work of this section.
B. Verify that installation of concrete forms, accessories, reinforcement, and embedded items is complete and that required inspections have been performed.
C. Do not proceed until unsatisfactory conditions have been corrected.
3.2 PREPARATION
A. Provide reasonable auxiliary services to accommodate field testing and inspections, acceptable to testing agency, including the following:
CAST-IN-PLACE CONCRETE 033000 - 15
1. Daily access to the Work.
2. Incidental labor and facilities necessary to facilitate tests and inspections.
B. Secure space for storage, initial curing, and field curing of test samples, including source of water and continuous electrical power at Project site during site curing period for test samples.
C. Security and protection for test samples and for testing and inspection equipment at Project site.
D. Formwork: Comply with requirements of ACI SPEC-301. Design and fabricate forms to support all applied loads until concrete is cured and for easy removal without damage to concrete.
E. Verify that forms are clean and free of rust before applying release agent.
F. Where new concrete is to be bonded to previously placed concrete, prepare existing surface by cleaning and applying bonding agent in according to bonding agent manufacturer's instructions.
1. Use epoxy bonding system for bonding to damp surfaces, for structural load-bearing applications, and where curing under humid conditions is required.
G. In locations where new concrete is doweled to existing work, drill holes in existing concrete, insert steel dowels and pack solid with non-shrink grout.
1. Lubricate or asphalt coat one-half of dowel bar length to prevent concrete bonding to one side of joint.
H. Interior Slabs on Grade: Install vapor retarder under interior slabs on grade. Comply with ASTM E1643. Lap joints minimum 6 inches (150 mm). Seal joints, seams and penetrations watertight with manufacturer's recommended products and follow manufacturer's written instructions. Repair damaged vapor retarder before covering.
3.3 INSTALLING REINFORCEMENT AND OTHER EMBEDDED ITEMS
A. Embedded Items: Place and secure anchorage devices and other embedded items required for adjoining Work that is attached to or supported by cast-in-place concrete.
1. Use setting drawings, templates, diagrams, instructions, and directions furnished with items to be embedded.
2. Install anchor rods, accurately located, to elevations required and complying with tolerances in of ANSI/AISC 303.
3. Install reglets to receive waterproofing and to receive through-wall flashings in outer face of concrete frame at exterior walls, where flashing is shown at lintels, shelf angles, and other conditions.
B. Fabricate and handle epoxy-coated reinforcing in accordance with ASTM D3963/D3963M.
C. Comply with requirements of ACI SPEC-301. Clean reinforcement of loose rust and mill scale, and accurately position, support, and secure in place to achieve not less than minimum concrete coverage required for protection.
D. Install welded wire reinforcement in maximum possible lengths, and offset end laps in both directions. Splice laps with tie wire.
CAST-IN-PLACE CONCRETE 033000 - 16
E. Verify that anchors, seats, plates, reinforcement and other items to be cast into concrete are accurately placed, positioned securely, and will not interfere with concrete placement.
3.4 PLACING CONCRETE
A. Before placing concrete, verify that installation of formwork, reinforcement, embedded items, and vapor retarder is complete and that required inspections are completed.
1. Immediately prior to concrete placement, inspect vapor retarder for damage and deficient installation, and repair defective areas.
2. Provide continuous inspection of vapor retarder during concrete placement and make necessary repairs to damaged areas as Work progresses.
B. Notify Architect and testing and inspection agencies 24 hours prior to commencement of concrete placement.
C. Do not add water to concrete during delivery, at Project site, or during placement unless approved by Architect in writing, but not to exceed the amount indicated on the concrete delivery ticket.
1. Do not add water to concrete after adding high-range water-reducing admixtures to mixture.
D. Before test sampling and placing concrete, water may be added at Project site, subject to limitations of ACI 301 (ACI 301M), but not to exceed the amount indicated on the concrete delivery ticket.
1. Do not add water to concrete after adding high-range water-reducing admixtures to mixture.
E. Place concrete in accordance with ACI PRC-304.
F. Place concrete for floor slabs in accordance with ACI PRC-302.1.
G. Deposit concrete continuously in one layer or in horizontal layers of such thickness that no new concrete is placed on concrete that has hardened enough to cause seams or planes of weakness.
1. If a section cannot be placed continuously, provide construction joints as indicated.
2. Deposit concrete to avoid segregation.
3. Deposit concrete in horizontal layers of depth not to exceed formwork design pressures and in a manner to avoid inclined construction joints.
4. Consolidate placed concrete with mechanical vibrating equipment in accordance with ACI
301 (ACI 301M).
a. Do not use vibrators to transport concrete inside forms.
5. Insert and withdraw vibrators vertically at uniformly spaced locations to rapidly penetrate placed layer and at least 6 inches (150 mm) into preceding layer.
6. Do not insert vibrators into lower layers of concrete that have begun to lose plasticity.
7. At each insertion, limit duration of vibration to time necessary to consolidate concrete, and complete embedment of reinforcement and other embedded items without causing mixture constituents to segregate.
CAST-IN-PLACE CONCRETE 033000 - 17
H. Deposit and consolidate concrete for floors and slabs in a continuous operation, within limits of construction joints, until placement of a panel or section is complete.
1. Do not place concrete floors and slabs in a checkerboard sequence.
2. Consolidate concrete during placement operations, so concrete is thoroughly worked around reinforcement and other embedded items and into corners.
3. Maintain reinforcement in position on chairs during concrete placement.
4. Screed slab surfaces with a straightedge and strike off to correct elevations.
5. Level concrete, cut high areas, and fill low areas.
6. Slope surfaces uniformly to drains where required.
7. Begin initial floating using bull floats or darbies to form a uniform and open-textured surface plane, before excess bleedwater appears on the surface.
8. Do not further disturb slab surfaces before starting finishing operations.
I. Finish floors level and flat, unless otherwise indicated, within the tolerances specified below.
3.5 JOINTING
A. Locate joints as indicated on drawings. Construct joints true to line, with faces perpendicular to surface plane of concrete. Coordinate with floor slab pattern and concrete placement sequence.
1. Install so strength and appearance of concrete are not impaired, at locations indicated on Drawings or as approved by Architect.
B. Place joints perpendicular to main reinforcement.
1. Continue reinforcement across construction joints unless otherwise indicated.
2. Do not continue reinforcement through sides of strip placements of floors and slabs.
C. Form keyed joints as indicated. Embed keys at least 1-1/2 inches (38 mm) into concrete.
D. Locate horizontal joints in walls and columns at underside of floors, slabs, beams, and girders and at the top of footings or floor slabs.
E. Use a bonding agent at locations where fresh concrete is placed against hardened or partially hardened concrete surfaces.
F. Use epoxy-bonding adhesive at locations where fresh concrete is placed against hardened or partially hardened concrete surfaces.
G. Anchor joint fillers and devices to prevent movement during concrete placement.
H. Control Joints in Slabs-on-Ground: Form weakened-plane control joints, sectioning concrete into areas as indicated. Construct control joints for a depth equal to at least one-fourth of concrete thickness as follows:
1. Grooved Joints: Form control joints after initial floating by grooving and finishing each edge of joint to a radius of 1/8 inch (3.2 mm). Repeat grooving of control joints after applying surface finishes. Eliminate groover tool marks on concrete surfaces.
2. Sawed Joints: Form control joints with power saws equipped with shatterproof abrasive or diamond-rimmed blades. Cut 1/8-inch- (3.2-mm-) wide joints into concrete when cutting
CAST-IN-PLACE CONCRETE 033000 - 18
action does not tear, abrade, or otherwise damage surface and before concrete develops random cracks.
I. Isolation Joints: Use preformed joint filler with removable top section for joint sealant, total height equal to thickness of slab, set flush with top of slab.
J. Isolation Joints in Slabs-on-Ground: After removing formwork, install joint-filler strips at slab junctions with vertical surfaces, such as column pedestals, foundation walls, grade beams, and other locations, as indicated.
1. Extend joint-filler strips full width and depth of joint, terminating flush with finished concrete surface unless otherwise indicated on Drawings.
2. Terminate full-width joint-filler strips not less than 1/2 inch (13 mm) or more than 1 inch (25 mm) below finished concrete surface, where joint sealants, specified in Section 079200 - Joint Sealants are indicated.
3. Install joint-filler strips in lengths as long as practicable. Where more than one length is required, lace or clip sections together.
3.6 FLOOR FLATNESS AND LEVELNESS TOLERANCES
A. Conform to ACI 117 (ACI 117M).
B. Minimum F(F) Floor Flatness and F(L) Floor Levelness Values:
1. Finish and measure surface so gap at any point between concrete surface and an unleveled, freestanding, 10-ft.- (3.05-m-) long straightedge resting on two high spots and placed anywhere on the surface does not exceed 1/8 inch (3 mm).
2. Exposed to View and Foot Traffic: F(F) of 25; F(L) of 20, on-grade only.
a. Minimum local values of flatness: F(F) of 17; and of levelness, F(L) of 15.
3. Under Thick-Bed Tile: F(F) of 20; F(L) of 15, on-grade only.
4. Under Carpeting: F(F) of 25; F(L) of 20, on-grade only.
5. Under Thin Resilient Flooring and Thinset Tile: F(F) of 35; F(L) of 25, on-grade only.
a. Minimum local values of flatness: F(F) of 24; and of levelness, F(L) of 17.
C. Measure F(F) Floor Flatness and F(L) Floor Levelness in accordance with ASTM E1155/E1155M, within 48 hours after slab installation; report both composite overall values and local values for each measured section.
D. Correct the slab surface if composite overall value is less than specified and if local value is less than two-thirds of specified value or less than F(F) 13/F(L) 10.
E. Correct defects by grinding or by removal and replacement of the defective work. Areas requiring corrective work will be identified. Re-measure corrected areas by the same process.
3.7 CONCRETE FINISHING
A. Repair surface defects, including tie holes, immediately after removing formwork.
B. Concrete Slabs: Finish to requirements of ACI PRC-302.1 and as follows:
CAST-IN-PLACE CONCRETE 033000 - 19
1. Trowel and Fine-Broom Finish: Apply a first trowel finish to surfaces indicated on Drawings or where ceramic or quarry tile is to be installed by either thickset or thinset method. While concrete is still plastic, slightly scarify surface with a fine broom perpendicular to main traffic route.
a. Coordinate required final finish with Architect before application.
b. Comply with flatness and levelness tolerances for trowel-finished floor surfaces.
2. Broom Finish: Apply a broom finish to exterior concrete platforms, steps, ramps, and locations indicated on Drawings.
a. Immediately after float finishing, slightly roughen trafficked surface by brooming with fiber-bristle broom perpendicular to main traffic route.
b. Coordinate required final finish with Architect before application.
3. Other Surfaces to Be Left Exposed/Sealed: Smooth trowel as described in ACI PRC- 302.1, minimizing burnish marks and other appearance defects.
3.8 CURING AND PROTECTION
A. Comply with requirements of ACI PRC-308. Immediately after placement, protect concrete from premature drying, excessively hot or cold temperatures, and mechanical injury.
1. Comply with ACI 301 (ACI 301M) and ACI 306.1 for cold weather protection during curing.
2. Comply with ACI 301 (ACI 301M) and ACI 305.1 (ACI 305.1M) for hot-weather protection during curing.
3. If evaporation rate in subparagraph below is exceeded, ACI 305R states that plastic shrinkage cracking is probable. See ACI 305R for estimated moisture-loss chart relating relative humidity, air and concrete temperature, and wind velocity to rate of evaporation.
4. Maintain moisture loss no more than 0.2 lb./sq. ft. x h (1 kg/sq. m x h), calculated in accordance with ACI 305.1,) before and during finishing operations.
B. Curing Formed Surfaces: Comply with ACI PRC-308 as follows:
1. Cure formed concrete surfaces, including underside of beams, supported slabs, and other similar surfaces.
2. Cure concrete containing color pigments in accordance with color pigment manufacturer's instructions.
3. If forms remain during curing period, moist cure after loosening forms.
4. If removing forms before end of curing period, continue curing for remainder of curing period, as follows:
a. Continuous Fogging: Maintain standing water on concrete surface until final setting of concrete.
b. Continuous Sprinkling: Maintain concrete surface continuously wet.
5. Absorptive Cover: Pre-dampen absorptive material before application; apply additional water to absorptive material to maintain concrete surface continuously wet.
a. Water-Retention Sheeting Materials: Cover exposed concrete surfaces with sheeting material, taping, or lapping seams.
b. Membrane-Forming Curing Compound: Apply uniformly in continuous operation by power spray or roller in accordance with manufacturer's written instructions.
1) Recoat areas subject to heavy rainfall within three hours after initial application.
2) Maintain continuity of coating and repair damage during curing period.
CAST-IN-PLACE CONCRETE 033000 - 20
C. Maintain concrete with minimal moisture loss at relatively constant temperature for period necessary for hydration of cement and hardening of concrete.
D. Surfaces Not in Contact with Forms: Comply with ACI PRC-308 as follows:
1. Initial Curing: Start as soon as free water has disappeared and before surface is dry. Keep continuously moist for not less than three days by water ponding, water-saturated sand, water-fog spray, or saturated burlap.
2. Final Curing: Begin after initial curing but before surface is dry.
3. Interior Concrete Floors:
a. Floors to Receive Floor Coverings Specified in Other Sections: Contractor has option of the following:
1) Absorptive Cover: As soon as concrete has sufficient set to permit application without marring concrete surface, install prewetted absorptive cover over entire area of floor.
(a) Lap edges and ends of absorptive cover not less than 12-inches (300-mm).
(b) Maintain absorptive cover water saturated, and in place, for duration of curing period, but not less than seven days.
4. Moisture-Retaining-Cover Curing: Cover concrete surfaces with moisture-retaining cover for curing concrete, placed in widest practicable width, with sides and ends lapped at least 12 inches…
This is the start of the file's text. The full file is on GovTribe.