This document is a detailed Statement of Work (SOW) for a hull inspection and zinc anode replacement service for the USCGC WILLIAM HART, a United States Coast Guard vessel located in Honolulu, Hawaii. The SOW requires a certified diver and support team to comprehensively inspect the underwater hull, propulsion systems, sea chests, and cathodic protection components, including detailed documentation using specific rating systems for paint deterioration and marine fouling. The contractor must produce both written and audio-video reports documenting the vessel's underwater condition, clean marine growth from surfaces, and replace zinc anodes, with specific requirements for video equipment, reporting, and inspection methodologies.
The related federal contract opportunity (Solicitation Number: 52000QR250011754) seeks a firm fixed-price quotation for this service, with quotes due by March 24, 2025 at 9:00 AM EST. Vendors must be registered in SAM.gov and submit a quote including cost breakdown, unit costs, total price, payment terms, and company information. The United States Coast Guard intends to award the contract based on best value, with the potential to award on an all-or-none basis. Quotations should be emailed to Timothy Ford and Stacy Spalding, with the work to be performed between April 7-14, 2025, at the Honolulu Coast Guard base.
View the file
Other files
| File | Type | Posted |
|---|---|---|
| FAR Clauses.pdf |
On GovTribe
Work with this file
- Download the original file
- Contacts named in this file
- Similar government files
- Ask GovTribe AI about this file
Text version
Hull Plating, U/W Body, Diver’s Inspect, Clean and Renew U/W Zinc Anodes Perform
1. SCOPE
1.1 Intent. This work item describes the requirements for the Contractor to conduct a hull inspection, cleaning of the vessel’s U/W body and renewal of U/W zinc anodes. Affected surfaces or components include, but are not limited to the following:
• U/W hull plating.
• U/W body coating system.
• Transducer(s)/sonar dome.
• Drive Systems
• Appendages
• Cathodic Protection
1.2 Government-furnished property.
MTI ITEM DESCRIPTION NSN/PN QTY
N Anode, B/T Gear Case P/N: 1081226, NIIN: 015485655 1 N Anode, B/T Tunnel P/N: : CM2000Z
NIIN: 200126334
N Anode, Sea Chest Grate P/N: GA-4, NIIN: 016476179 4 N Anode, Stern Tube P/N: Z0020202H3 REV. 0, NIIN:
016445483
N Nut, Self-Locking, P/N: 90715A145, NIIN:
015085774
N Screw, Prop Zinc Plate P/N: 950756, NIIN: 016340210 8 N Screw, Sea Chest Grate Anode P/N: 93190A634, NIIN:
016197182
N Screw, Stern Tube Covers P/N: 90585A626, NIIN:
016161107
N Zinc Plate, Propeller P/N: 950733, NIIN: 016278941 2
2. REFERENCES
OTHER REFERENCES
Code of Federal Regulations (CFR) Title 29, Part 1910, Subpart T, 2007, Commercial Diving Operations
3. REQUIREMENTS
3.1 General.
3.1.1 CIR.
None.
3.1.2 Tech Rep.
Not Applicable.
3.1.3
3.1.4 The Contractor must provide the Coast Guard Inspector 24 hours advance notice of when the diver inspection will occur. Before diving procedures are commenced, meet with the COR and the Coast Guard Inspector, to discuss diving safety requirements and the securing of cutter machinery, as applicable.
3.2 Pre-diving clearance. The Contractor must ensure that the diving team must obtain clearance from the Officer-of-the-Deck before beginning diving operations. Ensure the Coast Guard Inspector has capability for maintaining continuous two-way communication with diving personnel at all times, during the performance of this work item.
3.2.1 The Contractor must, in accordance with 29 CFR 1910.401-440, provide a certified diver and a tender team, as well as necessary support personnel and equipment, to accomplish the tasks specified herein.
3.3 Hull inspection requirements - general. The Contractor must survey the entire U/W body of the vessel to inspect for abnormal conditions or situations, which may include, but not be limited to the below-listed.
NOTE
At Contractor’s request, Ship’s force will secure and tag out the cathodic protection system, main engines, steering gear, generator set, A/C unit, fire pumps, and all other machinery which may cause a hazard while a diver is in the water.
WARNING
Mixed gas diving and live boating are not permitted.
• Hull plating and appendage damages.
• Coating system defects or failures.
• Welding corrosion and erosion.
• Deformation in appendages.
• Zinc performance.
3.3.1 Hull plating. The Contractor must inspect the exterior condition of the hull for presence of marine growth, deformation, and any evidence of major corrosion or electrolytic action. Inspect for deformation along the stem and keel areas, condition of butt-welded seams, doubler plates, lap seams, and any signs of damaged plating or unusual waviness in the plating.
3.3.2 Coating system inspection. The Contractor must inspect the condition of the U/W body coating system, for signs of the following:
• Peeling.
• Blistering.
• Abrasion.
3.3.2.1 Use the guidelines provided in Table I (Paint Deterioration Ratings (PDR) for Antifouling/Anticorrosion (AF/AC) Paint System) and Table 2 (Fouling Ratings (FR) In Order of Increasing Severity) to assist in proper documentation of the coating system degradation and fouling rate, respectively.
TABLE 1 - PAINT DETERIORATION RATINGS (PDR)
FORANTIFOULING/ANTICORROSION (AF/AC) PAINT SYSTEM
PAINT
DETERIORATION
RATING (PDR)
DESCRIPTION
10 AF paint intact, red in color or with mottled pattern of light green and red.
20 AF paint missing from edges, corners, seams welds, river or boll head to expose AC paint.
30 AF paint missing from slightly curved or flat areas to expose AC paint.
40 AF paint missing from intact blisters to expose AC paint.
50 AF blisters ruptured to expose intact AC paint.
60 AF/AC paint missing or peeling to expose steel substrate, no corrosion present.
70 AF/AC paint removed from edges, corners, seams, welds, river or bolt heads to expose steel substrate with corrosion present.
80 Ruptured AF/AC blisters on slightly curved or flat surfaces with corrosion stains present.
90 Area corrosion of steel substrate with no AF/AC paint cover due to peeling or abrasion damage.
100 Area corrosion showing visible surface evidence of pitting, scaling, and roughening or steel substrate.
TABLE 2 - FOULING RATINGS (FR) IN ORDER OF INCREASING SEVERITY
TYPE FOULING
RATING
(FR)
DESCRIPTION
Soft 0 A clean, foul-free surface; red and/or black AF paint or a bare metal surface.
Soft 10 Light shades of red and green (incipient slime). Bare metal and painted surfaces are visible beneath the fouling.
Soft 20 Slime as dark green patches with yellow or brown colored areas (advanced slime).
Bare metal and painted surfaces may by obscured by the fouling.
Soft 30 Grass as filaments up to 3 inches (76 mm) in length, projections up to 1/4 inch (6.4
mm) in height; or a flat network of filaments, green, yellow, or brown in color; or soft non calcareous fouling such as sea cucumbers, sea grapes, or sea squirts projecting up to 1/4 inch (6.4 mm) in height. The fouling cannot be easily wiped off by hand.
Hard 40 Calcareous fouling in the form of tubeworms I less than ¼ inch in diameter or height.
Hard 50 Calcareous fouling in the form of barnacles less than ¼ inch in diameter or height.
Hard 60 Combination of tubeworms barnacles, less I than ¼ inch (6.4 mm) in diameter or height.
Hard 70 Combination of tubeworms and barnacles, greater than ¼ inch in diameter or height.
Hard 80 Tubeworms closely packed together and growing upright away from surface.
Barnacles growing one on top of another, ¼ inch or less in height. Calcareous shells appear clean or white in color.
Hard 90 Dense growth of tubeworms with barnacles, ¼ inch or greater in height; Calcareous shells brown in color (oysters and mussels); or with slime or grass overlay.
Composite 100 All forms of fouling present, Soft and Hard, particularly soft sedentary animals without calcareous covering (tunicates) growing over various forms of hard growth.
3.3.3 Sea chests and other hull penetrations. The Contractor must accomplish the following:
• Inspect all sea chests and other hull penetrations for signs of any obstructions/marine growth in the openings that might prevent proper suction and discharge of water.
• Inspect for bare metal areas (surrounding penetrations) and for bare metal pitting.
• Inspect for general appearance, loose, damaged, or missing grates, loose or missing fasteners, condition of sea strainers and lockwire on bolt.
3.3.4 Propeller and shaft associated components. The Contractor must inspect the condition of the propeller shafts, struts, fairwaters, and rope guards. Note any loose or missing fairwater or rope guard fasteners.
3.3.4.1 Inspect propellers for corrosion, pitting, erosion, fouling, cracks, dings, curls, and nicks by side and blade.
3.3.4.2 Inspect the condition of the struts, keel drain plugs, rudders, rudder stocks, and rudder bearings, including any damage, pitting on leading and trailing edges of the rudder, and the presence of drain plugs.
3.3.5 Transducers. The Contractor must inspect the general condition of the fathometer transducer.
Record condition of rubber coating and amount of marine growth present. Note in the inspection report any cuts, gouges, or other surface defects found.
3.3.6 Cathodic protection system. The contractor must inspect the general condition and performance of the cathodic protection system. Record condition of zinc anodes on Table 7, Zinc Wastage.
3.4 Inspection documentation. The Contractor must document the hull survey as follows:
3.4.1 Written report. The Contractor must record the U/W body coating system fouling rating on the attached “Pre-Clean Bio-fouling Inspection Data” Form.
3.4.1.1 Note all inspection findings and observations, as applicable, on attached observations on the following attached inspection data forms, as applicable, on the attached : “Diver Hull Inspection Data” Form.
3.4.1.2 In addition to completing the ”Diver Hull Inspection Data” Form, do the following, as applicable:
• Document condition of running gear on attached “Running Gear Inspection Data” Form for each shaft.
• Document propeller condition on attached “Propeller Inspection Data” Form for each propeller.
• Document condition of rudders on attached “Port and Starboard Rudder Data Inspection” Form.
• Document condition of all U/W zincs on Table 7, Zinc Wastage.
3.4.2 Audio-video report. In addition to the written documentations specified above, The Contractor must produce an audio-video report, with narration, of all inspected surfaces. Place linear measuring devices, as applicable, in the field of view when videotaping hull damages, to provide scale for these damages.
3.4.3 Documentation submission. Within 24 hours after the completion of the diver inspection, The Contractor must do the following:
3.4.3.1 Submit a CFR indicating the amount of recommended U/W body surface cleaning, if any.
3.4.3.2 Submit both, the written and audio-video reports to the COR. Submit the audio-video report on two digital video discs (DVD) formatted to USCG requirements.
3.4.3.2.1 Ensure that all video equipment have the following characteristics/functions:
• Remote video/sound recorder.
• Suitability for underwater use.
• Auto-focus and auto-exposure.
• Color pictures.
• Two-way communication devices, to allow for communication and recording of communications between the diver operating the video camera and the Person-in-Charge, COR, and Coast Guard Inspector.
• Audio/visual cables long enough to transmit the video picture and two-way communications to the recorder and monitor.
• Online video monitor large enough, to allow the Person-in-Charge, the COR, and the Coast Guard Inspector to observe the video picture.
• Sufficient lighting to ensure a quality color video picture and depth of field.
• A yardstick or other suitable linear measuring device with clear measurement marks which can be read from the monitor.
3.4.3.2. 2 Closely monitor the video and sound quality during the survey, to ensure that the pictures on the monitor and the communication sounds remain of high quality. When either video or audio quality deteriorates, ensure that the survey is temporarily halted, until all problems have been corrected.
3.5. Hull cleaning requirements. Contractor must employ suitable means to clean the designated U/W body surfaces free of all marine growth, debris, and all other surface contaminants. The Contractor must ensure the following:
3.5.1 Ensure that existing U/W body coating system or non-coated surfaces do not incur any damage during cleaning process.
3.6 Renew UW Zinc Anodes. The contractor must renew U/W zinc anodes ensuring not to damage hull components during renewal process.
3.6.1 Document correct zinc and grate installation with photos included on final diver report.
4. NOTES
4.1 Unit responsibilities. The ship's force will tag-out systems in accordance with COMDINST M9077.1 (series) and MPC B10015.D including the below;
• All propulsion machinery and shafting, including auxiliary propulsion machinery such as the bow thruster, and all steering machinery whenever the diver is in the water.
• All underwater body transducers, including the sonar equipment, for the duration of the underwater inspection operation.
• All active cathodic protection equipment for the duration of the underwater inspection operation.
• Each sea suction while the diver is inspecting the sea suction's sea chest strainer.
4.2 Mailing of video record. Upon receipt, the EPO will retain the diver report and underwater video inspection locally and forward a copy to the Engineering Section of the Product Line Division to which the vessel is assigned.
4.3 MPC Completion. Cutter EPO is responsible for ensuring MPC’s B10015.D and B10018.D are properly completed and submitted.
4.4 Cutter POC. Cutter POC is Justin Graham, Engineering Petty Officer (907) 301-4953. Email: justin.l.graham@uscg.mil.
4.5 Period of performance must fall within 07APR2025– 14APR2025. Work to be performed at 400 Sand
Island Pkwy, Honolulu HI 96818 USA.
mailto:Christopher.c.giboney@uscg.mil
TABLE 3. PRE-CLEAN BIOFOULING INSPECTION DATA
PRE-CLEAN BIOFOULING INSPECTION DATA
VESSEL NAME: HULL TYPE / NUMBER LOCATION (CITY) DATE (mm/dd/yy)
PRODUCT LINE: INSPECTING ACTIVITY VISIBILITY (ft)
LOCATION OF LAST DRYDOCKING UNDOCKING DATE
LOCATION OF LAST PAINTING DATE
PAINT
TYPE: ANTIFOULING: ANTICORROSION:
DATE OF THE LAST WATERBORNE FULL HULL CLEANING DATE OF THE LAST WATERBORNE INTERIM CLEANING
UNDERWATER PHOTOGRAPHS TAKEN □ YES □ NO VIDEO TAKEN □YES □ NO
COMPONENTS ( CHECK IF: )
N/A NOT INSPECTED
( PERCENTAGES MUST ADD UP TO 100 )
FOULING RATING FOULING RATING FOULING RATING
PROPELLER Centerline FR- % FR- % FR- %
Port Outboard FR- % FR- % FR- %
Port Inboard FR- % FR- % FR- %
Starboard Inboard FR- % FR- % FR- %
Starboard Outboard FR- % FR- % FR- %
SHAFT Centerline FR- % FR- % FR- %
Port Outboard FR- % FR- % FR- %
Port Inboard FR- % FR- % FR- %
Starboard Inboard FR- % FR- % FR- %
Starboard Outboard FR- % FR- % FR- %
RUDDER Centerline FR- % FR- % FR- %
Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
SONAR DOME Port Side FR- % FR- % FR- %
Starboard Side FR- % FR- % FR- %
SEA CHEST Typical FR- % FR- % FR- %
BOW Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
SIDES Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
BOTTOM Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
STERN Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
TRANSOM Port FR- % FR- % FR- %
Starboard FR- % FR- % FR- %
Signature (Ship’s Engineer):
Signature (Diving Supervisor):
TABLE 4. DIVER HULL INSPECTION DATA
DIVER HULL INSPECTION DATA
VESSEL NAME: HULL TYPE / NUMBER LOCATION (CITY) DATE (mm/dd/yy)
PRODUCT LINE: INSPECTING ACTIVITY VISIBILITY (ft)
LOCATION OF LAST DRYDOCKING UNDOCKING DATE
LOCATION OF LAST PAINTING DATE
PAINT
TYPE: ANTIFOULING: ANTICORROSION:
DATE OF THE LAST WATERBORNE FULL HULL CLEANING
UNDERWATER PHOTOGRAPHS TAKEN □ YES □ NO
UNDERWATER WORK ACCOMPLISHED THIS DATE
□ FULL CLEAN □POLISH □MULTI-BRUSH
□INTERIM □HYDRO □HAND-HELD
DATE OF THE LAST WATERBORNE INTERIM CLEANING
UNDERWATER COLOR VIDEO TAKEN □ YES □ NO
□INSPECT □PAINT
□REPAIR □OTHER
1. HULL COATING SYSTEM (PDR )
a. ANTIFOULING PAINT
PERCENTAGE REMAINING
IS THE A/F □ HARD □ SOFT
PERCENT REJUVENATION
PERCENTAGE PEELING LOCALIZED or GENERAL BLISTERING LOCALIZED or GENERAL ABRASION LOCALIZED or GENERAL
CONDITION SUMMARY [ IF PAINT DAMAGE IS LOCALIZED, GIVE LOCATION(s) ]
b) ANTICORROSION PAINT
PERCENTAGE REMAINING
PERCENTAGE PEELING LOCALIZED or GENERAL BLISTERING LOCALIZED or GENERAL ABRASION LOCALIZED or GENERAL
c) DOCKING BLOCK AREAS (PDR )
AVERAGE PERCENTAGE OF BLOCK AREAS PAINTED %
BARE METAL PITTING % IN. DIAMETER IN. DEEP
TABLE 5. DIVER HULL INSPECTION DATA (CONT.)
DIVER HULL INSPECTION DATA (CONTINUED)
2. CATHODIC PROTECTION SYSTEM
a. SACRIFICIAL ANODES (ZINCS)
AVERAGE PERCENTAGES OF ANODES REMANING %
ANODES ARE: □ UNIFORMLY WASTED □WASTAGE GREATEST IN FOLLOWING AREAS:
ANODES ARE : □WELDED □BOLTED □ BOTH
NUMBER AND LOCATION OF ANY ANODES MISSING OR INACTIVE:
MISSING
INACTIVE
b. IMPRESSED CURRENT
□ DAMAGE NOTED ON ATTACHED DRAWING (Port/Stbd) (FRAME )
□WIRES LOOSE, BROKEN, OR MISSING (Port/Stbd) (FRAME )
□CAPASTIC SHIELD DAMAGE (Port/Stbd) (FRAME )
□ INSULATORS LOOSE OR DAMAGED (Port/Stbd) (FRAME )
□ OTHER (Port/Stbd) (FRAME )
3. GENERAL HULL DAMAGE (HULL PLATING, BILGE KEELS, etc.):
4. HULL PENETRATIONS (PDR )
% CLOGGED WITH MARINE GROWTH (POST CLEAN)
% BARE METAL (AREA SURROUNDING PENETRATION)
% BARE METAL PITTING
AVERAGE PIT SIZE: in. DIAMETER, in. DEPTH
CONDITION SUMMARY:
TABLE 6. DIVER HULL INSPECTION DATA (CONT.)
DIVER HULL INSPECTION DATA (CONTINUED)
5. SONAR DOME
□ NO VISIBLE DAMAGE □ DAMAGE NOTED ON ATTACHED DRAWING □CUTS □LAYER SEPARATION □WIRE PILES EXPOSED
6. PROPULSION SHAFTING
VISIBLE BARE METAL □ YES □ NO RUST BLEEDING □ YES □NO PITTING □ YES □NO
CONDITION SUMMARY (TYPE OF DAMAGE, LOCATION AND SIZE):
7. STRUTS AND BEARING HOUSING
PERCENT BARE METAL: STARBOARD PORT
MAIN % %
INTERMEDIATE % %
PDR
CONDITION OF STRUT LEADING AND TRAILING EDGES:
CONDITION OF ROPE GUARDS:
CONDITION OF FAIRWATERS:
8. RUDDER
CONDITION SUMMARY:
9. PROPELLERS
PROP #1: NICKS □ NO DAMCAUGRELS□ DAMAGE SHOWN ONCRAATCTKASC–HELADRDGREASWT ICNRGASCK LENGTH in.
PROP #2: NICKS CURLS CRACKS – LARGEST CRACK LENGTH in.
PROP #3: NICKS CURLS CRACKS – LARGEST CRACK LENGTH in.
PROP #4: NICKS CURLS CRACKS – LARGEST CRACK LENGTH in.
PROPELLERS NUMBERED STARBOARD TO PORT.
Diving Supervisor:
Ship’s Engineer:
□ NO DAMAGE □ DAMAGE SHOWN O
STARBOARD
ATTACHED DRAWINGS
PORT
PERCENT BARE METAL % %
PDR
ACCESS PLATES INTACT? □ YES □ NO □ YES □ NO
WAS RUDDER SOUNDED? □ YES □ NO □ YES □ NO
ANY SIGNS OF FLOODING? □ YES □ NO □ YES □ NO
ANY SIGNS OF DROPPING? □ YES □ NO □ YES □ NO
TABLE 7. ZINC WASTAGE
FIGURE 1. PROPELLER INSPECTION DATA
FIGURE 2. STARBOARD RUNNING GEAR INSPECTION
FIGURE 3. PORT AND STARBOARD RUDDER INSPECTION
| 1. SCOPE |
| 2. REFERENCES |
| OTHER REFERENCES |
| 3. REQUIREMENTS |
| TABLE 1 - PAINT DETERIORATION RATINGS (PDR) FORANTIFOULING/ANTICORROSION (AF/AC) PAINT SYSTEM |
| 4. NOTES |
| TABLE 3. PRE-CLEAN BIOFOULING INSPECTION DATA |