Next Generation Materials for Armor Piercing (AP) Small Caliber Projectiles
Closed Solicitation Posted
- Solicitation number
- A16-067
- Agency
-
PEO Ammunition
Acquisition Support Center, Department of Defense
- Responses due
- Set-aside
- Total Small Business
Opportunity facts
- NAICS code
- 541715 Research and Development in the Physical, Engineering, and Life Sciences (except Nanotechnology and Biotechnology)
- More information
Notice details come from DoD SBIR/STTR (DSIP). Updated .
Notice text
DoD SBIR topic A16-067
Component: ARMY
Command: PEO AMMO
Phase: SBIR Program Phase I Action
Technology Areas: Weapons
Keywords: super hard; tungsten carbide; tungsten heavy alloy; net shape; armor piercing; penetrator; bullet; small caliber
Objective:
Develop novel material technologies to replace the current tungsten carbide solution that will meet density and hardness requirements with the objective of reducing the manufacturing cost of the small caliber armor piercing projectile.
Description:
The current process of machining tungsten carbide rod stock takes 15 minutes per penetrator. Using current (mostly manual) machining methods, completed penetrators are forecasted to cost about $21 each which is an order of magnitude higher than desired. Current penetrators are typically composed of cemented tungsten carbide due to the material’s high density and hardness. However, the metallic binder (traditionally cobalt) that cements the tungsten carbide together often reduces these properties of interest in the bulk component. This effort is seeking a materials solution to develop a high density, high hardness material replacement that can be fabricated into a cost-effective ammunition package. The proposed technology must be amenable to mass production in order to meet annual ammunition buys on the order of millions per year. Key material properties include a density greater than 15 g/cc and a minimum hardness of 2500 HVN, post machining. Envelope dimensions per item are 0.25” in diameter and 2.00” in length. Final per unit cost, post machining, should be no more than $1.00 per piece. Other metrics (such as a measure of toughness, grain size, binder composition, and dimensional tolerances) will depend on the proposed solution and will be addressed during Phase I and II of this SBIR
Phase I:
During Phase I, a feasibility study of the proposed material concept(s) shall be conducted to provide evidence that demonstrates they can meet the stated requirements. This study should identify the equipment and resources needed to prototype the proposed material(s), as well as initial material concept(s) and unit cost estimates, with sufficient rationale. The phase 1 deliverable is a final report and engineering analysis, to include the plan to build and test the prototype in Phase II.
Phase II:
Phase II shall begin by prototyping the material(s) and evaluating its performance against the stated requirements. It is expected that one or more design iterations will occur during the 2nd phase. Phase II will end with a proof-of-concept prototype tested to demonstrate the properties and producibility of the material(s). Deliverables include monthly progress reports, material samples, a manufacturing plan, and a final report, including product cost data.
Phase III:
Phase III shall begin with the execution of the manufacturing plan developed in Phase II. Continued development shall be pursued to increase yields and reduce manufacturing costs.
Files
| File | Type | Posted |
|---|---|---|