AF191-026: Crack Sizing from Vibrothermography Nondestructive Inspection (NDI) Image

PROJECTED CMMC LEVEL REQUIREMENT:

N/A

TECHNOLOGY AREAS:

Materials

MODERNIZATION PRIORITIES:

KEYWORDS:

Vibrothermography, Sonic IR, POD, crack sizing, NDI, NDE, imaged data

ADDITIONAL INFORMATION

OBJECTIVE:

Develop, demonstrate, and validate a method to estimate the size of cracks from imaged data generated from Vibrothermography

DESCRIPTION:

Vibrothermography Nondestructive Inspection (NDI), also known as Sonic Infrared (IR) inspection, is beginning to be recognized as a viable whole-field method for detection of fatigue-like cracks or flaws in metallic turbine engine components. Like Florescent Penetrant Inspection (FPI), the present method for assessing Nondestructive Evaluation (NDE) system capability by Vibrothermography is hit/miss which produce only qualitative information as to the presence or absence of a flaw. While this is sufficient for inspection of some turbine engine components, the Air Force (AF) wishes to expand the usefulness of Vibrothermography to fracture critical life limited turbine engine components. The FAA is also presently investigating the use of Vibrothermography for turbine engine disk inspection for civil aviation. With these components, the (AF) Depot inspection interval is determined by the available crack propagation margin, in engine cycles, determined from a given inspectable flaw size. Therefore the ability to accurately, reliably, and with high confidence estimate the size of the crack is an absolute necessity. It is beyond the scope of this document to provide a primer on fracture mechanics and the interrelationship with inspection crack size to determine crack propagation margin of fracture critical turbine engine components. The offeror is expected to show comprehensive understanding of this topic and this knowledge is a significant evaluation factor for any proposal submitted to this solicitation. The current state-of-the-art production inspection methods used for detection of surface breaking cracks or flaws at the AF Depot are FPI and Eddy Current Inspection (ECI). The capability of an FPI system is often defined to a specified crack size, typically 0.035 inches deep by 0.070 inches long surface crack with a 90/95 probability of detection (POD). So, while FPI cannot provide a crack size, the capability of an FPI system is such that any positive indication using the FPI method is at least a 0.035” x 0.070” or larger. When fracture mechanics demands a smaller detectable flaw size, ECI is the method of choice. Since ECI capability is determined from specimen data, it provides some quantitative measure of the size of the flaw typically at a 90/50 POD. ECI starts at the FPI limit 0.035” x 0.070”, with the lower limit being a function of many variables, with the most important being geometry. In general for simple flat geometries, ECI can detect cracks as small as 0.005 inches deep by 0.010 inches long surface crack. Since the pass or reject decision for fracture critical turbine engine components is based on an estimated inspected crack or flaw size, in order for Vibrothermography to be useful as an alternate to FPI or ECI, it must also be capable to estimate the inspected crack or flaw size. The government will not provide any materials, specimens, or components, equipment data, or facilities during this effort. It will be the responsibility of the proposer to identify a vendor to perform Vibrothermography testing.

PHASE I:

Create low cycle fatigue (LCF) cracks in flat plate of any nickel-base superalloy of choice, crack size approximately

0.035 inches deep by 0.070 inches long. Develop and demonstrate method to estimate size of cracks from imaged data generated from Vibrothermography. Metrics for success is estimate within 25% of actual in length and/or depth. Verify ground truth through destructive characterization.

PHASE II:

Create low cycle fatigue (LCF) cracks in flat plate as well as a geometry resembling the leading edge of an airfoil of any nickel-base superalloy of choice, with crack size approximately 0.020 inches deep by 0.040 inches long. Mature the method from Phase 1 to estimate with statistical metrics of accuracy the size of cracks from imaged data generated from Vibrothermography. Metrics for success is to estimate within 10% of actual in length and/or depth for both geometries. Verify ground truth through destructive characterization.

PHASE III DUAL USE APPLICATIONS:

Additional maturation and refinement as necessary for more complex geometries and crack sizes with improved estimation, and validation of the method. Market tool as a standalone package or integrate into a commercial package such as COMSOL or VibroSim. These packages are examples only.

REFERENCES:

Quantifying the vibrothermographic effect, Stephen D. Holland, Christopher Uhl, Zhong Ouyang, TomBantel, Ming Li, William Q. Meeker, John Lively, Lisa Brasche, David Eisenmann, NDT&E International 44 (2011) 775–782

1.

Physics-based image enhancement for infrared thermography, Stephen D. Holland , Jeremy Renshaw, NDT&E International 43 (2010) 440–445

2.

TECHNICAL POINT OF CONTACT (TPOC):

None

File details come from the government source that posted it. Updated .