AF182-014: Non-Destructive Testing for Landing Gear Applications

PROJECTED CMMC LEVEL REQUIREMENT:

N/A

TECHNOLOGY AREAS:

Materials

MODERNIZATION PRIORITIES:

KEYWORDS:

NDI, Landing Gear, Coatings

ADDITIONAL INFORMATION

OBJECTIVE:

Find anomalies on High Strength Steel & High Strength Aluminum Landing Gear components without removing coatings. Anomalies include but not limited to cracks, poor coating adhesion, substrate surface non-uniformity from grit blast/peening, subsurface corrosion, heat damage (grinding burns), bearing stiction, fretting, etc.

DESCRIPTION:

Landing Gear (LG) are specialized structures designed to sustain the high stresses and loads of landing aircraft.

The geometries of LG are generally rounded and complex making it difficult for ‘standard’ probes to accomplish NDT. Some LG parts are made of High Strength Steels (HSS). During manufacture, rework, or surface grinding/finishing there is the potential that HSS LG parts are overheated resulting in an under/over tempered martensitic condition (burn). Another type of anomaly is when the coatings (i.e. Chrome plate or High Velocity Oxygen Fuel (HVOF) coatings) dis-bond from the substrate, whether from corrosion or a weak initial bond. Other LG parts are made from high strength aluminum alloys. The common anomalies to be detected are corrosion, pitting, cracks, stress corrosion cracking, etc. Please note the detection of anomalies required is not limited to the ones described above. A multitude of NDT techniques are used to detect the anomalies in landing gear parts see TOs 4B-1-32, 4S-1-182 and 4W-1-61. The current NDT techniques often require the removal of coatings and or are in efficient / non reliable. Also, LG are designed to a safe life criteria, meaning that NO cracks are allowed, so, ideally, if the detection limits for such anomalies could be reduced, i.e., find pre-crack flaws, that would allow the removal of the LG component prior to a catastrophic fracture. During the manufacturing and or rework process most LG parts undergo shot peening prior to coatings application. The uniformity of the shot peen is currently determined via coupon tests that are supposed to relate to the appropriate criteria. A method to validate the appropriate levels of peening would be invaluable. This topic is to research and develop a thermographic NDT technique that can detect undesirable material conditions to include, but not limited to cracks, poor coating adhesion, substrate surface non-uniformity due to grit blast and peening, subsurface corrosion, coating-to-substrate interface contaminants, and heat damage from grinding burns, bearing stiction, high load bearing fretting, etc. Since there are a number of cylinders or cylinder shaped geometries used in LG, the minimum Inner Diameter (ID) to consider/test is as small as 0.5” and the minimum Outer Diameter (OD) is 0.75. The maximum Inner Diameter (ID) to test on is 12” and the maximum Outer Diameter (OD) is 13”. As noted, LG are designed to a safe life criteria thereby the minimum detection size would ideally be pre-crack indications. Detection of corrosion and/or de-bonds of 0.25” diameter or smaller is the preferred goal.

PHASE I:

Develop a solution that meets above requirements and conduct preliminary business case analysis (BCA) to determine implementation costs, including a return-on-investment (ROI) calculation that compares anticipated savings to expected costs. Proof-of-concept prototype(s) shall be developed to demonstrate conformance to the requirements.

PHASE II:

Initiate and complete the test plan developed in Phase I. Proof-of-concept prototype(s) shall be refined to installation-ready article and shall undergo testing to verify and validate all requirements. The new technique(s) should provide as good or better inspection resolution with less ambiguity than the current methods of gear inspections. This should include the aforementioned of not having to remove coatings and/or inefficiencies and reliabilities. This process may require multiple iterations before a final design is selected. Refine BCA/ROI based on the final design.

PHASE III DUAL USE APPLICATIONS:

If cost effective, transition and implement the verified and validated technology.

REFERENCES:

TO 4W-1-61, TECHNICAL MANUAL, MAINTENANCE AND OVERHAUL INSTRUCTIONS ALL TYPE AIRCRAFT

WHEELS, 1 NOVEMBER 2017

1.

SAE-AMS-2430, Shot Peening, Automatic, Issued 1948-09, Revised 2015-012.

TO 4S-1-182, TECHNICAL MANUAL, GENERAL OVERHAUL AND MAINTENANCE INSTRUCTIONS AIRCRAFT

LANDING GEAR AND COMPONENTS, 20 SEPTEMBER 2017

3.

TO 4B-1-32, TECHNICAL MANUAL, MAINTENANCE AND OVERHAUL INSTRUCTIONS ALL TYPE AIRCRAFT

BRAKES, 27 DECEMBER 2017

4.

TECHNICAL POINT OF CONTACT (TPOC):

None

File details come from the government source that posted it. Updated .