TECH DATA- CLOTH HERITAGE GREEN ELASTIQUE 564 PGC 12169.pdf

PDF 95 KB Posted

Attached to
Cloth, AGSU Heritage Green Shade 564 Elastique, 55/45 Poly/Wool Federal contract opportunity
Solicitation number
SPE1C122R0018
Issued by
Defense Logistics Agency Troop Support Clothing and Textiles

View the file

Other files for this federal contract opportunity

Other files attached to Cloth, AGSU Heritage Green Shade 564 Elastique, 55/45 Poly/Wool, newest first.
File Type Posted
GL-PD 19007A.pdf PDF

On GovTribe

Work with this file on GovTribe

  • Download the original file
  • Contacts named in this file
  • Similar government files
  • Ask GovTribe AI about this file

Text version

CLOTH, ELASTIQUE HERITAGE GREEN 564 POLY/WOOL 55%/45% CLASS 1 UNTREATED

TEXT ID ST LANGUAGE E RP001:

DLA PACKAGING REQUIREMENTS FOR PROCUREMENT RA001: THIS DOCUMENT

INCORPORATES TECHNICAL AND/OR QUALITY REQUIREMENTS (IDENTIFIED BY AN 'R'

OR AN 'I' NUMBER) SET FORTH IN FULL TEXT IN THE DLA MASTER LIST OF

TECHNICAL AND QUALITY REQUIREMENTS FOUND ON THE WEB AT:

http://www.dla.mil/HQ/Acquisition/Offers/eProcurement.aspx

FOR SIMPLIFIED ACQUISITIONS, THE REVISION OF THE MASTER IN EFFECT ON THE

SOLICITATION ISSUE DATE OR THE AWARD DATE CONTROLS. FOR LARGE

ACQUISITIONS, THE REVISION OF THE MASTER IN EFFECT ON THE RFP ISSUE DATE

APPLIES UNLESS A SOLICITATION AMENDMENT INCORPORATES A FOLLOW-ON

REVISION, IN WHICH CASE THE AMENDMENT DATE CONTROLS.

CLOTH, ELASTIQUE, POLY/WOOL GL-PD 19007A CLASS 1 UNTREATED HERITAGE GREEN

564 8.7 OZ

NOTE: All references to Certification Labeling and Procedures in the document do not apply to this procurement. RP001: DLA PACKAGING

REQUIREMENTS FOR PROCUREMENT RQ009: INSPECTION AND ACCEPTANCE AT ORIGIN

RQ011: REMOVAL OF GOVERNMENT IDENTIFICATION FROM NON-ACCEPTED SUPPLIES

ELASTIQUE, CLASS 1 UNTREATED HERITAGE GREEN 564 8.7 OZ HERITAGE GREEN 564

TYPE I, MOTHPROOFED, STANDARD SAMPLE IS IDENTIFIED AS ROLL NO 3958.

ADDITIONAL INFORMATION FOR PD 19007 Dated 15 July 2019: STANDARD SAMPLE

FOR HERITAGE GREEN 564 IS IDENTIFIED AS ROLL NO 3958 AND IS APPLICABLE

FOR SHADE, FINISH AND COLORFASTNESS.

CHANGES TO GL-PD-19007A;

CLOTH, ELASTIQUE, POLYESTER AND WOOL

Paragraph 2.3, under “AMERICAN ASSOCIATION OF TEXTILE CHEMISTS AND COLORISTS (AATCC)”, line 3: Delete “AATCC Evaluation Procedure 5” and its title.

Paragraph 3.6, TABLE I, under “Requirement” for “Weight, oz./sq. yd.”: Delete “8.7 (± 0.3)” and substitute “8.5 (± 0.3)”.

Paragraph 3.8, line 2, after “standard sample”: Add a period and delete remainder of sentence.

Paragraph 3.8.1: Delete the second sentence in its entirety.

Paragraph 3.9: Delete and substitute the following new paragraph:

“3.9 Pilling. The cloth shall be processed to show a rating of not less than “4” using the ASTM Photographic Rating Standard. Testing shall be as specified in 4.4.6.”

Paragraph 3.12: Delete in its entirety.

ADD THE FOLLOWING NEW PARAGRAPH:

http://www.dla.mil/HQ/Acquisition/Offers/eProcurement.aspx

“4.4.3.1 LIMITS OF SLUBS AND KNOTS. ONLY SLUBS AND KNOTS WHICH EXCEED “D”

OR 3-1/2 AS APPLICABLE, FOR SLUBS AND “C” FOR KNOTS ON THE SEARS FABRIC

DEFECT SCALE SHALL BE SCORED (SEE 6.6).”

Pargraph 4.4.6, TABLE IV, Line 21: Delete Characteristic for “Finish” and all information pertaining to it.

Line 30: Delete Characteristic for “Fabric appearance rating” and all information pertaining to it.

TABLE IV: Delete footnote 5/ in its entirety.

DISTRIBUTION STATEMENT A. Approved for public release. Distribution is unlimited

THE CLOTH SHALL BE MOTHPROOFED IN ACCORDANCE WITH MIL-C-43665C, DATED 14

NOVEMBER 1986. (Ref. 17354).

ADDITIONAL INFORMATION FOR PPP-P-1132C: PPP-P-1132C PACKAGING OF WOOLEN,

WORSTED AND WOOL BLEND. PPP-P-1132 HAS BEEN CANCELLED. USE ASTM-D-3951-

STANDARD PRACTICE FOR COMERCIAL PACKAGING. COPIES MAY BE OBTAINED FROM

THE AMERICAN SOCIETY FOR TESTING AND MATERIALS, 100 HARBOR DRIVE, WEST

CONSHOHOCKEN, PA. 19428.

ADDITIONAL INFORMATION FOR MIL-C-43665: INTERIM SPECIFICATION CHANGES TO

MIL-C-43665C:

PAGE 2, PARA. 3.2, LINE 2, AFTER "TABLE 1 " INSERT "OR TABLE 1A", PAGE 3,

TABLE 1, DELETE "SODIUM (4,5-DICHLORO, 2-CHLOROMETHANE SULFONAMIDO) 3',4'

6',TRICHLORO) DISHENYL ETHER (SEE 6.3.2) 0.26 0.60". .

PAGE 3, AFTER TABLE 1, INSERT THE FOLLOWING NEW TABLE: "TABLE 1A,

MOTHPROOFING COMPOUND. % ON WEIGHT OF WOOL. MOTHPROOFING COMPOUND

MIN. MAX. EDOLAN ETS BEFORE DRYCLEANING *(3-PHENOXYPHENYL) METHYL

PLUS OR MINUS CIS/TRANS 3-(2-,2- DICCHLOROETHENYL)2,2-

DIMETHYLCYCLORPPANECARBOXYLATE. 0.058 0.40 CIS/TRANS RATIO:MAX.55%

PLUS OR--AFTER DRY-CLEAN MINUS CIS AND MIN.PLUS OR MINUS

TRANS.(*PERMETHRIN) 0.029 0.40 .

PAGE 3,PARA.3.4, LINE 3, AFTER "3.2" INSERT "TABLE 1". . PAGE 3, AFTER

PARA. 3.4 INSERT NEW PARAGRAPH AS FOLLOWS: "3.4.1 PERCENT OF MOTHPROOFING

COMPOUND. THE PERCENTAGES OF MOTHPROOFING COMPOUND SPECIFIED IN TABLE

1A SHALL BE BASED ON WEIGHT OF PURE COMPOUND ON THE WOOL FIBER CONTENT

WHEN TESTED BY HIGH PERFORMANCE LIQUID CHROMATOGRAPH (HPLC) METHOD,

OBTAINABLE FROM BAYER CORP., ROCK HILL, SC 29732 (SEE 4.2.2)".

PAGE 5, PARAGRAPH 4.2.2,TABLE 11,DELETE THE FOLLOWING: CHARACTERISTIC

REQUIREMENT TEST . PARAGRAPH METHOD "SODIUM (4,5-DICHLORO 2-CHLORO-

METHANE SULFONAMIDO)3',4',6', TRICHLORO) DIPHENYL ETHER 3.4 4.3.1

3/ 4/" AND SUBSTITUTE THE FOLLOWING: CHARACTERISTIC REQUIREMENT

TEST . PARAGRAPH METHOD "EDOLAN ETS *(3-PHENOXYPHENYL

3.4.1 HPLC 7/ METHYL PLUS OR MINUS CIS/TRANS 3-(2,2-

DICHLOROETHENYL) 2,2-DIMETHYL-CYCLOPROPANECARBOXYLATE CIS/TTRANS RATIO:

MAX.55% PLUS OR MINUS CIS AND MIN. PLUS OR MINUS TRANS. *(PERMRTHRIN)" .

PAGE 5, PARAGRAPH 4.2.2, FOR CHARACTERISTIC EDOLAN ETS,UNDER TEST METHOD

COLUMN, ADD FOOTNOTE "7"/,ADD NEW FOOTNOTE "8"/.

PAGE 6, PARAGRAPH 4.2.2, TABLE II.AFTER FOOTNOTE "7/",ADD THE

FOLLOWING:"8"/ THE SAMPLE SHALL BE DRY-CLEANED FOR THREE CYCLES IN

ACCORDANCE WITH AATCC TEST METHOD 86 BEFORE DETERMINING MOTHPROOFING

COMPOUND CONTENT. . PAGE 6, PARA.4.2.2, TABLE 11, AFTER FOOTNOTE 6/,

INSERT "7/ HIGH PERFORMANCE LIQUID CHROMATOGRAPHY (HPLC) TEST METHOD MAY

BE OBTAINED FROM BAYER CORP., ROCK HILL, SC 29732." .

PAGE 6, PARAGRAPHS 4.3,4.3.1,4.3.1.1,4.3.1.2, 4.3.1.3,4.3.1.4,4.3.1.5

DELETE PARAGRAPHS IN THEIR ENTIRETY WITH NO REPLACEMENT. .

PAGE 7, PARAGRAPHS 4.3.1.6, 4.3.1.7, 4.3.1.7.1 DELETE PARAGRAPHS IN THEIR

ENTIRETY WITH NO REPLACEMENT.

PAGE 8, PARAGRAPHS 4.3.1.7.2, 4.3.1.8, 4.3.1.8.1 DELETE PARAGRAPHS IN

THEIR ENTIRETY WITH NO REPLACEMENT.

PAGE 9, PARAGRAPHS 6.3 2, 6.4, 6.5, 6.6 DELETE PARAGRAPHS IN THEIR

ENTIRETY WITH NO REPLACEMENTS.

PAGE 11, DELETE FIGURE 1 IN ITS ENTIRETY WITH NO REPLACEMENT.

PAGE 5 TABLE II, UNDER TEST METHOD: DELETE "2015" AND SUBSTITUTE "2015.3"

NOTE! MITTEN FF CONC. SUPPLIED BY CIBA-GEIGY CORP. P.O. BOX 11422,

GREENSBORO, NC 27409 . EDOLAN ETS, SUPPLIED BY MILES INC.MOBAY ROAD,

PITTSBURGH,PA.15205-9741. . ARE APPROVED MOTH PROOFING AGENTS FOR

MILITARY FABRICS. (Ref. T1118)

ADDITIONAL INFORMATION FOR MIL-I-45208: NOTE: MIL-I-45208 HAS BEEN

CANCELLED AND REPLACED BY THE FOLLOWING: INTERNATIONAL STANDARDS ISO

9001:2008 OR AMERICAN SOCIETY FOR QUALITY ASQ 2008 VERSION. (ref. T1286 )

ADDITIONAL INFO FOR FED-STD-4 GLOSSARY OF FABRIC IMPERFECTIONS: REVISION

B: 7/29/64; AMENDMENT 2: 9/12/75 NOTICE 1, DATED 10/1/87. DEV. TO FED.

STD. 4B & AM. 2, PAGE 2, SEC.I.

PARA. 2.1. IN IMPERFECTION COMMERCIAL TERMINOLOGY AND GLOSSARY NO.

COLUMNS, AFTER SHADE BAR - 14 INSERT: "SHADED CLOTH-61B". PAGE 8 PARA.

3.4, GLOSSARY NO. "61A- OFF SHADE", IN "DEFINITION" COLUMN, DELETE ":

SHADED SIDE TO SIDE, SIDE TO CENTER OR END TO END". ADD NEW GLOSSARY NO.

"SHADED CLOTH "61B-SHADED CLOTH (SHADED SIDE TO SIDE, SIDE TO CENTER OR

END TO END) WITH THE FOLLOWING DEFINITION: "COLOR DIFFERENCE BETWEEN THE

RESPECTIVE CLOTH AREAS".

PAGE 22, SECTION III, PARAGRAPH 2.1, IN "IMPERFECTION COMMERCIAL

TERMINOLOGY" AND GLOSSARY NO." COLUMNS, AFTER "SHADE BAR-15" INSERT:

"SHADED CLOTH - 62A"

PAGE 27, PARAGRAPH 3.4, GLOSSARY NO. "62-OFF SHADE" IN "DEFINITION"

COLUMN DELETE: "SHADED SIDE TO SIDE, SIDE TO CENTER OR END TO END". ADD

NEW GLOSSARY NO, "62A-SHADED CLOTH (SHADED SIDE TO SIDE, SIDE TO CENTER

OR END TO END)" WITH THE FOLLOWING DEFINITION: "COLOR DIFFERENCE BETWEEN

THE RESPECTIVE CLOTH AREAS." DEVIATION FROM FED. STD. 4B, AND AMEND 2: PG

2, SECTION 1, PARA.2.1, IN "IMPERFECTION COMMERCIAL TERMINOLOGY" AND

"GLOSSARY NUMBER" COLUMNS, AFTER "SHADE BAR-14",INSERT: "SHADED CLOTH

61B".

PG 8, PARA.3.4, GLOSSARY NUMBER "61A-OFF SHADE" IN "DEFINITION" COLUMN,

DELETE, "SHADED SIDE TO SIDE, SIDE TO CENTER OR END TO END". ADD NEW

GLOSSARY NO."61B SHADED CLOTH "SHADED SIDE TO SIDE, SIDE TO CENTER OR END

TO END" WITH THE FOLLOWING DEFINITION; "COLOR DIFFERENCE BETWEEN THE

RESPECTIVE CLOTH AREAS."

PAGE 22, SECTION III, PARAGRAPH 2.1, IN "IMPERFECTION COMMERCIAL

TERMINOLOGY" AN GLOSSARY NO." COLUMNS, AFTER "SHADE BAR-15" INSERT:

"SHADED CLOTH - 62A"

PAGE 27, PARAGRAPH 3.4, GLOSSARY NO "62-OFF SHADE" IN "DEFINITION" COLUMN

DELETE: "SHADED SIDE TO SIDE, SIDE TO CENTER OR END TO END". ADD NEW

GLOSSARY NO, "62A-SHADED CLOTH (SHADED SIDE TO SIDE, SIDE TO CENTER OR

END TO END)" WITH THE FOLLOWING DEFINITION: "COLOR DIFFERENCE BETWEEN THE

RESPECTIVE CLOTH AREAS." Ref. T0202 - 04/04/07)

ADDITIONAL INFORMATION FOR FED-STD-191: FED-STD-191A NOTICE 7, DATED

AUGUST 9, 2000 IS HEREBY INACTIVE FOR NEW DESIGN. WHEN NOT USING FED-

STD-191, SEE INTERIM CHANGES TO END ITEM SPECIFICATION FOR REPLACEMENT

ASTM.

INTERIM CHANGES TO FED-STD-191A:

TEST METHOD 5202, PARA. 5.3, DELETE FIRST SENTENCE AND SUBSTITUTE: "THE

SPECIMEN SHALL BE CLAMPED FIRMLY, WITH ONE END FLUSH WITH THE OUTER EDGE

OF THE VISE, SUCH THAT ONE INCH OF SPECIMEN LIES WITHIN THE CLAMP AND ONE

INCH OF THE SPECIMEN EXTENDS BEYOND THE CENTER OF ROTATION (FACE OF THE

VISE), AND WITH THE LONG EDGE PARALLEL TO THE FACE OF THE DIAL PLATE".

TEST METHOD 5309.1 ABRASION RESISTANT OF TEXTILE WEBBING. PAGE 1, PARA

4.1.2, LINE 4: DELETE "B-97" AND SUBSTITUTE "B-91". THE FOLLOWING METHODS ARE

IDENTIFIED AS SPECIFYING OZONE DEPLETING SUBSTANCES: 1100, 1200, 1240,

1400, 1410, 1500, 1510,1520,1530, 1540, AND 1550. PARA 5.1 OF THESE TEST

METHODS REQUIRE THE USE OF 1,1,1- TRICHLOROETHANE, ALCOHOL OR ETHER.

1,1,1-TRICHLORETHANE IS AN OZONE DEPLETING SUBSTANCE (METHYL CHLOROFORM)

AND IS THEREFORE PROHIBITED. THE USE OF EITHER ALCOHOL OR ETHER IS

REQUIRED WHEN THESE METHODS ARE IN BASIC OR ANY REFERENCED DOCUMENT.

METHOD 5202, STIFFNESS OF CLOTH, DIRECTIONAL; CANTILEVER BENDING METHOD.

PAGE 2, PARA. 5.3 DELETE FIRST SENTENCE AND SUBSTITUTE WITH THE

FOLLOWING: "THE SPECIMEN SHALL BE CLAMPED FIRMLY, WITH 1 END FLUSH WITH

THE OUTER EDGE OF THE VISE, SUCH THAT 1" OF THE SPECIMEN LIES WITHIN THE

CLAMP AND 1" OF THE SPECIMEN EXTENDS BEYOND THE CENTER OF ROTATION (INNER

FACE OF THE VISE) AND WITH THE LONG EDGE PARALLEL TO THE FACE OF THE DIAL

PLATE."

METHOD 5556.1, MOBILE LAUNDRY EVALUATION FOR TEXTILE MATERIALS,

PAGE 5, PARA. 5.2.2, LINE 8: DELETE SENTENCE BEGINNING WITH "THE

SPECIMENS AND BALLAST" IN ITS ENTIRETY AND SUBSTITUTE WITH THE FOLLOWING:

"THE SPECIMENS AND BALLAST SHALL BE SEPARATED, OPENED TO FULL WIDTH AND

PLACED IN A PRE-HEATED DRYER HAVING A STACK TEMPERATURE OF 140-180 DEG.

F. THIS TEMPERATURE RANGE CORRESPONDS TO A SETTING OF "HIGH" ON THE

TEMPERATURE INDICATOR ON THE DRYER. DRYING SHALL CONTINUE FOR 45-60

MINUTES OR UNTILSAMPLES ARE DRY IN A ROTATING TUMBLE DRYER."

PAGE 5, PARA.5.2.3, LINE 8: DELETE SENTENCE BEGINNING WITH "THE SPECIMENS

AND BALLAST" IN ITS ENTIRETY AND SUBSTITUTE WITH THEFOLLOWING: "THE

SPECIMENS AND BALLAST SHALL BE SEPARATED, OPENED TO FULL WIDTH AND PLACED

IN A PRE-HEATED DRYER HAVING A STACKTEMPERATURE OF 140-180 DEG. F. THIS

TEMPERATURE RANGE CORRESPONDS TO A SETTING OF "HIGH" ON THE TEMPERATURE

INDICATOR ON THE DRYER. DRYING SHALL CONTINUE FOR 35-40 MINUTES OR UNTIL

SAMPLES ARE DRY."

METHOD 5931, ELECTROSTATIC DECAY OF FABRICS; DETERMINATION OF PAGE 1,

PARA. 3: AFTER NUMBER OF DETERMINATIONS ADD "PER SAMPLE UNIT". PAGE 1,

PARA. 4: DELETE "APPARTUS" AND SUBSTITUTE "APPARATUS". PAGE 1, PARA.

5.1, LINE 3: AFTER "AT" DELETE"APPROXIMATELY".

PAGE 2, PARA. 5.2, LINES 2, AND 5: AFTER "OF" ADD "+-".

LINE 6: AFTER "TO" ADD "+-". PAGE 2, PARA. 5.3: DELETE IN ITS ENTIRETY

AND SUBSTITUTE WITH THE FOLLOWING:"5.3 MOUNT A SPECIMEN TIGHTLY ACROSS

THE ELECTRODES, CENTERING IT OVER THE SENSOR OPENING. THE SURFACE OF THE

TEST SPECIMEN (BACK OR FRONT) SHALL FACE THE SENSOR. RECORD (OPTIONAL)

THE RESIDUAL CHARGE LEVEL ON THE SAMPLE AS SEEN BY THE SENSOR, INCLUDING

POLARITY. NOTE THAT TEST SAMPLES WITH THE RESIDUAL CHARGE LEVELS OF LESS

+500 VOLTS YIELD THE BEST RESULTS. APPLY +5000 VOLTS TO THEELECTRODES

FOR A PERIOD OF 20 SECS. AT THE END OF THE 20 SECOND PERIOD, THE HIGH

VOLTAGE (5000 VOLTS) SHALL BE TURNED OFF ANDTHE SPECIMENS IMMEDIATELY

GROUNDED. THE VOLTAGE BEHAVIOR OF THE SPECIMEN WITH RESPECT TO TIME

SHALL BE PLOTTED ON THE RECORDER. NOTE: IN SOME CASES, THE TEST EQUIPMENT

WILL DISPLAY VOLTAGE AND DECAY TIME INFORMATION AND A CHART RECORDER IS

NOT NECESSARY."

PAGE 2, PARA. 5.4, LINE 3: DELETE SENTENCE BEGINNING WITH "IF THE

SPECIMEN DID" IN ITS ENTIRETY.

PAGE 2, PARA. 5.5: DELETE PARAGRAPH IN ITS ENTIRETY AND SUBSTITUTE WITH

THE FOLLOWING: "RECORD THE MAXIMUM VOLTAGE LEVEL(INCLUDING POLARITY) AND

DECAY TIME TO 10% OF THE MAXIMUM VOLTAGE LEVEL ACHIEVED."

PAGE 2, PARA. 5.6, LINE 1: ADD THE FOLLOWING PRIOR TO 1ST SENTENCE:

"REVERSE VOLTAGE POLARITY REPEAT MEASUREMENT, ANDRECORD RESULTS."

PAGE 3, PARA. 6.6: DELETE PARAGRAPH IN ITS ENTIRETY AND SUBSTITUTE WITH

THE FOLLOWING: "THE AVERAGE TIME TO DECAY TO 10%OF THE MAX VOLTAGE SHALL

BE INCLUDED FOR EACH OF THE WARP & FILLING DIRECTIONS, AS WELL AS THE

OVERALL AVERAGE, FOR EACHFABRIC TESTED. THESE WILL BE OBTAINED BY

AVERAGING THE TEST RESULTS (ABSOLUTE VALUE OF) TOGETHER FOR BOTH

VOLTAGEPOLARITIES. UNLESS OTHERWISE STATED IN THE REQUIREMENTS DOCUMENT,

THE FABRIC SHALL BE CONSIDERED ACCEPTABLE IF THEAVERAGE MAXIMUM VOLTAGE

IN BOTH THE WARP AND FILLING DIRECTIONS IS LESS THAN 4000 VOLTS, AND THE

AVERAGE DECAY TIME (TO 10% MAXVOLTAGE) IS GREATER THAN 0.5 SECONDS IN

BOTH THE WARP AND FILLING DIRECTIONS. IT SHALL BE INDICATED WHETHER THE

FABRIC ISACCEPTABLE OR NON-ACCEPTABLE."

PAGE 3, PARA. 7.1, SECOND COLUMN, LINE 2: DELETE 406C AND SUBSTITUTE WITH

"406D".

AFTER PARA. 7.1, ADD THE FOLLOWING: "7.2 NOTE: IF THE MODEL 406D STATIC

DECAY METER, OR EQUIVALENT, IS USED, A CHART RECORDER ISNOT MANDATORY FOR

THE TEST." (Ref. T0215)

INSPECTION OF SUPPLIES SHALL BE IN ACCORDANCE WITH FAR PART 52.246-2

STANDARD INSPECTION.

ADDITIONAL INFORMATION FOR MIL-STD-105E: MIL-STD-105E, dated 10 May 1989, is hereby canceled. Future acquisitions may refer to: MIL-STD-1916, "DoD Preferred Methods for Acceptance of Product," or ANSI/ASQ Z1.4, "Sampling Procedures and Tables for Inspection by Attributes." Users are cautioned to evaluate these documents for their particular application before citing it as a replacement document.

(Copies of MIL-STD-1916 are available online at http://assist.daps.dla.mil or from the Standardization Document Order Desk, 700 Robbins Avenue, Building 4D, Philadelphia, PA 19111-5094.)

(Copies of ANSI/ASQ Z1.4 are available online at www.asq.org or ASQ Distribution Center, 5131 S. Third Street, Milwaukee, Wisconsin 53207- 6028.)

MIL-STD-129R - DEPARTMENT OF DEFENSE STANDARD PRACTICE MILITARY MARKING

FOR SHIPMENT AND STORAGE DATED 18 FEBRUARY 2014

INTERIM CHANGES: OMISSION OF MARKINGS ON EXTERIOR SHIPPING CONTAINERS OF

ITEMS IN THE DLA TROOP SUPPORT CLOTHING AND TEXTILE (C&T) DIRECTORATE:

THE NOMENCLATURE AND MANUFACTURER'S NAME (WHEN THE NAME IDENTIFIES THE

MATERIAL) SHALL BE OMITTED FROM ALL EXTERIOR SHIPPING CONTAINERS OF DLA

TROOP SUPPORT C&T ITEMS, REGARDLESS OF MODE OF SHIPMENT.

IF THE MANUFACTURER'S NAME DOES NOT IDENTIFY THE MATERIAL AS BEING

CLOTHING, IT MAY REMAIN. NSNS SHALL BE SHOWN ON ALL SHIPPING CONTAINERS

OF C&T ITEMS, THE PACKING LIST SHALL BE PLACED INSIDE THE LAST CONTAINER

TO BE LOADED FOR EACH SHIPMENT. THE WORDS "PACKING LIST HERE" SHALL BE

STENCILED, NOT HAND LETTERED, ON THE CONTAINER.

MIL-STD-147E w/CHANGE 1 23 December 2013 SUPERSEDING MIL-STD-147E 16 May

DEPARTMENT OF DEFENSE STANDARD PRACTICE PALLETIZED UNIT LOADS ADDITIONAL

INFORMATION FOR MIL-STD-655D:.

INTERIM CHANGES TO MIL-STD-655D:

PAGE 3, PARA 4.1, ADD "QUALITY LEVEL 7".

PAGE 5, TABLE I, UNDER QUALITY LEVEL"7", ADD UNDER ENTIRE SAMPLE "7

POINTS PER 100 SQ. YARDS", ADD UNDER INDIVIDUAL ROLLS "10 POINTS PER 100

SQ. YDS." (Ref. T0319) THE DEMERIT POINTS PER 100 SQ YDS SHALL NOT EXCEED

A QUALITY LEVEL 12 IAW

File details come from the government source that posted it. Updated .