SPMYM2-22-1330 (ADDITIONAL ORDERING DATA) COPPER NICKEL PLATES.pdf

PDF 130 KB Posted

Attached to
COPPER NICKEL PLATES Federal contract opportunity
Solicitation number
SPMYM2-22-Q-1330
Issued by
Defense Logistics Agency Land and Maritime

View the file

Other files for this federal contract opportunity

Other files attached to COPPER NICKEL PLATES, newest first.
File Type Posted
SPMYM2-22-Q-1330 (SOLICITATION) COPPER NICKEL PLATES.pdf PDF

On GovTribe

Work with this file on GovTribe

  • Download the original file
  • Contacts named in this file
  • Similar government files
  • Ask GovTribe AI about this file

Text version

MATERIAL ORDERING DATA

MIL-C-15726

IDN: N4523A 2088-1090

ICN: 38RTC16301 KO: S03 KOI: 006

Paragraph 6.2 Ordering Data

Preparer's note: Forgings previously procured to this specification are now procured to MIL- C-24679.

a. MIL-C-15726F, Copper-Nickel Alloy, Sheet, Plate, Strip, Bar, Rod and Wire dated 25 October 1988; including Amendment 1, dated 8 October 1991

b. Current issue of DODISS is to be cited in the solicitation.

c. Composition: Alloy C71500 (formerly 70-30) Form: plate Temper: M20-soft

d. Is a specific manufacturing technique required? If yes, specify: No

3.1 Unless otherwise specified, material shall be finished by such hot working, cold working, or heat treatment as may be necessary to meet the properties specified.

e. Dimensions: 5/8"thk, 76-1/2" x 107"

3.7 Unless otherwise specified, tolerances shall be specified in FED-STD-146.

3.7.1 When specified, tolerances shall be all plus or all minus.

f. Is alloy identity test required? No

3.9.2 When specified, each random mill length, prior to cutting to ordered length, and each forging shall be shown to be of the correct generic metallurgical group after final marking.

g. Is sampling for visual and dimensional inspections other than specified? If yes, specify: No

4.2.4 Sampling shall be as specified.

6.7 Unless otherwise specified (see 4.2.4), sampling should be in accordance MIL-STD-105, general inspection level II, acceptable quality level 1.5.

h. Is nondestructive inspection required? If yes, specify: No

4.2.5 Liquid penetrant inspection shall be in accordance with MIL-STD-271.

i. Is liquid penetrant inspection other than specified? If yes, specify: No

4.3.3.2 Liquid penetrant inspection shall be in accordance with MIL-STD-271. (Amendment 1)

j. Method used for alloy identity test: NA

4.5.1 Method of test for alloy identity shall be by an approved procedure.

k. Level of packing and packaging: C, Special marking is not required

5.1 The material shall be packaged to level A or C; packed to level A, B, or C, as specified and marked in accordance with MIL-C-3993.

Additional Data Requirements: NA Prepared By: Alexis Gahan

Code: 260.3

MATERIAL ORDERING DATA

MIL-C-15726

IDN: N4523A 2088-1091

ICN: 38RTC16301 KO: S03 KOI: 007

Paragraph 6.2 Ordering Data

Preparer's note: Forgings previously procured to this specification are now procured to MIL- C-24679.

a. MIL-C-15726F, Copper-Nickel Alloy, Sheet, Plate, Strip, Bar, Rod and Wire dated 25 October 1988; including Amendment 1, dated 8 October 1991

b. Current issue of DODISS is to be cited in the solicitation.

c. Composition: Alloy C71500 (formerly 70-30) Form: plate Temper: M20-soft

d. Is a specific manufacturing technique required? If yes, specify: No

3.1 Unless otherwise specified, material shall be finished by such hot working, cold working, or heat treatment as may be necessary to meet the properties specified.

e. Dimensions: 1-1/4"thk, 80" x 91"

3.7 Unless otherwise specified, tolerances shall be specified in FED-STD-146.

3.7.1 When specified, tolerances shall be all plus or all minus.

f. Is alloy identity test required? No

3.9.2 When specified, each random mill length, prior to cutting to ordered length, and each forging shall be shown to be of the correct generic metallurgical group after final marking.

g. Is sampling for visual and dimensional inspections other than specified? If yes, specify: No

4.2.4 Sampling shall be as specified.

6.7 Unless otherwise specified (see 4.2.4), sampling should be in accordance MIL-STD-105, general inspection level II, acceptable quality level 1.5.

h. Is nondestructive inspection required? If yes, specify: No

4.2.5 Liquid penetrant inspection shall be in accordance with MIL-STD-271.

i. Is liquid penetrant inspection other than specified? If yes, specify: No

4.3.3.2 Liquid penetrant inspection shall be in accordance with MIL-STD-271. (Amendment 1)

j. Method used for alloy identity test: NA

4.5.1 Method of test for alloy identity shall be by an approved procedure.

k. Level of packing and packaging: C, Special marking is not required

5.1 The material shall be packaged to level A or C; packed to level A, B, or C, as specified and marked in accordance with MIL-C-3993.

Additional Data Requirements: NA Prepared By: Alexis Gahan

Code: 260.3

File details come from the government source that posted it. Updated .