DWG_1420-0312_Supplement.docx
DOCX document 14 KB Posted
- Attached to
- Steel Machining Fixture Federal contract opportunity
- Solicitation number
- N6449819Q5211
About this file
Drawing Supplemental Information
View the file
Other files for this federal contract opportunity
| File | Type | Posted |
|---|---|---|
| Amendment_0002.pdf | ||
| DWG_1420-0312_Supplement.docx | DOCX document | |
| Amendment_0001.pdf | ||
| DWG_1420_0312_CLB-BSS_Machining_Fixture.pdf | ||
| N6449819Q5211.pdf |
On GovTribe
Work with this file on GovTribe
- Download the original file
- Contacts named in this file
- Similar government files
- Ask GovTribe AI about this file
Text version
DWG 1420-0312 Supplement for BSS Machining Fixture Naval Foundry and Propeller Center
The following information shall be considered included as a supplement to DWG 1420-0312.
1. Machining and Fabrication Note Sheet Locations:
- Machining tolerance - see Sheet 1
- Fabrication - Note 101 and Sheet 6
2. B/M sheet 4 calls for 145.0" OD, which is the raw material size (finish machine later).
3. Top and Bottom plates machining Tolerance:
- Finished machine size is shown in VIEW 8-4A and VIEW 8-2A as Ø144.0"
- Machining tolerance - See Sheet 1
4. Sheet 8 calls for flatness and II within 002":
- Overall height requirement is 17.500/17.750
- Equal material removal from both sides (within +/-.125'' tolerance).
5. Surface finish:
- Machining surface RMS - See Sheet 1
- Fabrication/Flame cut - No need to consider surface finish
6. There is a typo error on sheet 7 detail view 7-2A drawing. Only 8 supports are required
7. There are no Painting or Finishing Requirements for the assembly.
8. ID Tag Fastening and location on assembly:
- See VIEW 8-2A and Detail View 8-1C
- Fastened with B/M item 11. See View 4-3A and Detail View 4-1A
9. For Stress Relieving assembly after fabrication step 2 (sheet 7) and before any machining, follow these steps:
a. Place the weldment flat inside the furnace. Furnace temperature shall not exceed 800°F at the time the weldment is placed in it.
b. Heat the weldment at a rate no greater than 200°F per hour from 800°F to 1200°F
c. Hold 1200°F for three hours
d. Cool furnace at a rate less than 200°F per hour to 800°F. Air cool to ambient temperature.
10. Required plate cannot be welded from 2 separate plates to create the required 120” diameter. Plate must be one piece.