Attachment 1 SPMYM324Q4063.pdf

PDF 157 KB Posted

Attached to
Rod, Plastic Federal contract opportunity
Solicitation number
SPMYM324Q4063
Issued by
Defense Logistics Agency Land and Maritime

About this file

This document appears to be the technical specifications and requirements for a contract to manufacture Delrin AF DE 588 plastic rods in accordance with certain NAVSEA drawings and standards. The key details include:

The rods must meet specific material property requirements for features like density, melting point, tensile strength, and dimensional stability. Detailed test methods are provided to verify these properties. The rods must also contain 18-23% Teflon fiber content. The item has a stock number of 9330-LL-L01-0021 and a size of 6.00" diameter +/- 0.250". Data requirements include mechanical property test reports, certificates of compliance, and safety data sheets. Preservation, packaging, and inspection requirements are also specified.

The related federal contract opportunity is for a solicitation to procure these plastic rods, with a solicitation number of SPMYM324Q4063. The procuring agency is the Defense Logistics Agency Land and Maritime.

View the file

Other files for this federal contract opportunity

Other files attached to Rod, Plastic, newest first.
File Type Posted
Data Requirements 4063.pdf PDF
Combined Synopsis Solicitation Rod Plastic SPMYM324Q4063.docx DOCX document
FAR-DLAD-Local Notes and Clauses 4063.docx DOCX document

On GovTribe

Work with this file on GovTribe

  • Download the original file
  • Contacts named in this file
  • Similar government files
  • Ask GovTribe AI about this file

Text version

CONTRACT

PRINTED 7/11/2024 ATTACHMENT PAGE

9330 1L

C DESCRIPTION/SPECIFICATIONS

C.1 MANUFACTURE DELRIN AF DE 588 IN ACCORDANCE WITH NAVSEA DWG

803-4384678 REV C AND DRN 4384678 C2, GENERAL NOTES 7.C.(9) AND 7.D

WITH ALL ITS APPLICABLE NOTES EXCEPT AS AMPLIFIED OR MODIFIED HEREIN:

ITEM PROPERTY ASTM TEST METHOD (L/R) VALUE

(A) SPECIFIC GRAVITY D792 (NOTE 1) 1.50-1.57

(B) MELTING POINT D2133 0R D3418 172-184 DEG C (342-363 DEG F)

(C) TENSILE STRENGTH (MIN) D638 (NOTES 1 & 4) 6100 LB/SQ. IN

(D) TENSILE IMPACT (MIN) D1822 TYPE S (NOTES 1 & 4) 5 FT-LB/SQ. IN.

(E) COMPRESSIVE STRESS D695 2100 @ 1% DEF.

(MIN PSI) (NOTES 1 & 4) 11,000 @ 10% DEF.

(F) WATER ABSORPTION D570 .30% MAX 24 HOURS

(G) ROCKWELL HARDNESS (R) D785 (NOTE 1) 115 +/- 15

(H) TEFLON FIBER CONTENT (NOTE 2) 18-23%

(I) DIMENSIONAL CHANGE (NOTE 3) .7% MAX

NOTES:

1. MATERIAL CONDITIONING PRIOR TO TEST IS AT THE VENDOR'S OPTION.

2. TEFLON FIBER CONTENT- AS CERTIFIED BY DUPONT. WHITE TEFLON

INCLUSIONS SHALL NOT EXCEED THE FOLLOWING:

A. DIAMETER 1/32"

B. LENGTH 1/8"

ITEM NO.

STOCK NUMBER

9330-LL-L01-0021

SPECIAL CHARACTERISTICS

SIZE:6.00" DIAM + 0.250" /- 0.00"

ITEM NAME PLASTIC ROD, ROUND, ( DELRIN AF DE 588 )

SECTION B

SMIC

9G

1 1 OF 3

9330 1L

C. DENSITY 6 INDICATIONS PER 100 SQ. IN.

3. THE TEST METHOD TO DETERMINE DIMENSIONAL STABILITY SHALL BE PERFORMED

AS FOLLOWS: THE TEST SPECIMENS (FINISHED PIECES) TESTED SHALL BE MEASURED

AT 23 +/- 3 DEG C (73 +/- 5 DEG F) AND PLACED IN A MINERAL OIL* BATH MAINTAINED AT 160 +/- 3 DEG C (320 +/- 5 DEG F). THE SPECIMENS SHALL REMAIN IN THE BATH FOR SIX

(6) HOURS AT TEMPERATURE AND ALLOWED TO SLOW COOL IN THE BATH AT A RATE

NOT TO EXCEED 23 +/- 3 DEG C (73 +/- 5 DEG F) PER HOUR. WHEN THE BATH REACHES

23 +/- 3 DEG C (73 +/- 5 DEG F), THE TEST SPECIMENS SHALL BE REMOVED AND MEASURED.

THE PERCENT CHANGE IN EACH DIMENSION, OUTSIDE DIAMETER, INSIDE DIAMETER,

AND THICKNESS, SHALL NOT BE GREATER THAN THE VALUE SPECIFIED. IN LIEU OF FINISHED PIECES FOR TEST SPECIMEN PREPARE A 1.5 IN. LONG SLICE (FULL DIAMETER) TO USE AS TEST SPECIMEN AND

TEST AS REQUIRED.

* MINERAL OIL MEETS THE SPECIFICATION AS LISTED BELOW:

DESCRIPTION……………………………………………PASSES U.S.P. TEST (USP XX, P.1143)

SOLUBILITY………………………………………………PASSES U.S.P. TEST (USP XX, P.1143)

NEUTRALITY……………………………………………PASSES U.S.P. TEST (USP XX, P.532)

READILY CARBONIZABLE SUBSTANCES…..PASSES U.S.P. TEST (USP XX, P.532)

LIMIT OF POLYNUCLEAR COMPOUNDS…….PASSES U.S.P. TEST (USP XX, P.532)

SOLID PARAFFIN………………………………………PASSES U.S.P. TEST (USP XX, P.532)

SPECIFIC GRAVITY @ 25DEG C (77DEG F) ..O.8600 TO 0.8900

VISCOSITY @ 37.8 DEG C (100 DEG F)……….73.6 TO 84.4 CENTISTOKES (340-390 SUS)

FLASH POINT CLEVELAND OPEN CUP………..216 DEG C (420 DEG F) (TYPICAL)

REFRACTIVE INDEX @ 20 DEG C (68 DEG F).1.480 (TYPICAL)

4. VALUES ARE MINIMUM MEAN VALUES. INDIVIDUAL SPECIMEN VALUES MAY NOT VARY MORE THAN 25% BELOW THE SPECIFIED MINIMUM MEAN VALUE. SHOULD ONE SPECIMEN EXCEED THE 25% CRITERIA, RETEST IS REQUIRED. FAILURE TO MEET THE ABOVE CRITERIA A SECOND TIME IS CAUSE FOR REJECTION.

C.2 DATA REQUIREMENTS:

C.2.1 TEST REPORTS (MECHANICAL PROPERTY TEST), SEE EXHIBIT A, SEQUENCE A001

C.2.2 CERT. OF COMPLIANCE, SEE EXHIBIT A, SEQUENCE A002

C.2.3 SAFETY DATA SHEETS, SEE EXHIBIT A, SEQUENCE A003

C.2 C500 MERCURY CONTROL (SUPPLIES)

D PRESERVATION/PACKAGING/PACKING

D.1 D4 PREPARATION FOR DELIVERY (COMMERCIALLY PACKAGED ITEMS)

E INSPECTION ACCEPTANCE

1 2 OF 3

9330 1L

E.1 E1 RESPONSIBILITY FOR INSPECTION

H SPECIAL PROVISIONS

K Section

L Section

M Section

1 3 OF 3

File details come from the government source that posted it. Updated .